Title: The effects of different silane crosslinking approaches on composites of polyethylene blends and wood flour

Source: Journal of Applied Polymer Science, Volume 120, 2292-2303 (2011)

Author(s)Clemons, Craig M.; Sabo, Ronald C.; Hirth, Kolby C.

Publication Year: 2011  View PDF »

Category: Journal Articles
Associated Research Project(s):   FPL-4706-2A

Abstract: Though silane chemistry has been used to crosslink unfilled polyethylene for many years, such crosslinking has only been recently applied to wood plastic composites to improve properties such as creep resistance. However, the presence of wood significantly changes the silane chemistry and a greater understanding is necessary for optimal processing and performance. We investigated three different approaches of adding silane and peroxide during reactive extrusion of wood-plastic composites were investigated and compared to their unfilled counterparts. Up to 2 grams of a 20:1 solution of vinyltrimethoxysilane and dicumyl peroxide by weight were added per 100 grams of plastic. Low density polyethylene, high density polyethylene, and a blend of the two were investigated as matrices in composites containing approximately 25% wood flour. The unfilled plastics crosslinked efficiently and little premature crosslinking occurred during processing. Though only modest improvements in tensile strengths were found in unfilled plastics, the notched Izod impact energy of unfilled HDPE improved nearly 600% when crosslinked. Unlike the unfilled plastics, most of the crosslinking of the composites occurred during processing. This resulted in high viscosities and processing difficulties, negating some of the advantages of a separate crosslinking step and limiting the amount of crosslinking possible. Some reinforcement of the plastics by the wood flour was achieved when sufficient crosslinking solution was added. Adding crosslinking solution also and greatly increased reverse-notched impact energies. The differences between the approaches for preparing the crosslinked composites appeared to largely be a matter of efficiency in terms of the amount of crosslinking solution required to affect processing and performance. The most efficient approach was a two-step procedure where the silane was first grafted to the plastic and then wood flour was compounded with the grafted silane in a second step. Published 2010 Wiley Periodicals, Inc. J Appl Polym Sci 120: 2292-2303, 2011

Keywords: Composite materials; mechanical properties; injection molding of plastics; thermoplastic composites; plastics; extrusion; wood-plastic composites; silane; testing; extrusion process; crosslinking; polyethylene; wood flour; materials; creep; peroxides; dicumyl peroxide; impact testing; viscosity; recycled products; wood-plastic materials; biocomposites; HDPE; high density polyethylene; vinyltrimethoxysilane; strength; tensile strength; Izod test; reactive extrusion

Publication Review Process: Formally Refereed

File size: 1 kb(s)

Date posted: 10/17/2011

This publication is also viewable on Treesearch:  view
RITS Product ID: 40122
Current FPL Scientists associated with this product (listed alphabetically)
Clemons, Craig M.
Materials Research Engineer
Sabo, Ronald C.
Research Materials Engineer
 

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »