Title: Cellulose nanomaterials review: structure, properties and nanocomposites

Source: Chem. Soc. Rev., 2011, 40, 3941-3994; 2011

Author(s)Moon, Robert J.; Martini, Ashlie; Nairn, John; Simonsen, John; Youngblood, Jeff

Publication Year: 2011  View PDF »

Category: Journal Articles
Associated Research Project(s):   FPL-4707-3A

Abstract: This critical review provides a processing-structure-property perspective on recent advances in cellulose nanoparticles and composites produced from them. It summarizes cellulose nanoparticles in terms of particle morphology, crystal structure, and properties. Also described are the self-assembly and rheological properties of cellulose nanoparticle suspensions. The methodology of composite processing and resulting properties are fully covered, with an emphasis on neat and high fraction cellulose composites. Additionally, advances in predictive modeling from molecular dynamic simulations of crystalline cellulose to the continuum modeling of composites made with such particles are reviewed (392 references).

Keywords: Nanostructured materials, nanotechnology, technological innovations, microstructure, cellulose, chemistry, composite materials, nanocomposites, nanocrystals, crystallization, chemical composition, biocomposites, nanoparticles, mechanical properties, suspensions, elasticity, surface chemistry, nanocellulose, crystalline cellulose, nanocomposites, crystallinity, review article, bacterial cellulose, synthesis paper

Publication Review Process: Formally Refereed

File size: 3 kb(s)

Date posted: 07/12/2011

This publication is also viewable on Treesearch:  view
RITS Product ID: 39097
Current FPL Scientist associated with this product
Moon, Robert J.
Materials Research Engineer
  

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »