Title: Salt Damage To Wood, 'Fuzzy Wood' Often Confused with Fungal Decay

Source: USDA Forest Service, Forest Products Laboratory, Techlines, 2011

Author(s)Kirker, Grant; Glaeser, Jessie;

Publication Year: 2011  View PDF »

Category: TechLines

Abstract: Many types of deterioration can affect wood in service. One potential problem facing dock owners is the occasional development of 'fuzzy wood' caused by salt uptake into the wood (Fig. 1). This salt damage - also referred to as 'salt kill' or salt defibration - is sometimes seen in wood that is chronically exposed to salt, such as marine pilings, bridge decks where salt is used as a de-icer, utility poles that are splashed with road salt, or wood associated with salt storage.

Keywords: Wood biodegradation; docks; wood poles; wood moisture; moisture; deterioration; salt; rock salt; sea salt; saline waters; seawater; durability; wood decay; timber bridges; wooden bridges; saltwater; sea water; poles; fuzzy wood

Publication Review Process: Non-Refereed (Other)

File size: 1,217 kb(s)

Date posted: 07/05/2011
RITS Product ID: 39217
Current FPL Scientist associated with this product
Kirker, Grant
Research Forest Products Technologist
  

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »