Title: Full-scale shear wall tests for force transfer around openings

Source: In: Proceedings of the international council for research and innovation in building and construction--working commission W18--timber structures. 2010 Augsut 22-26. Nelson, New Zealand. Karisruhe, Germany: Karisruhe institute of Technology. 9 p. (published on CD excluding page numbers)

Author(s)Skaggs, Tom.; Yeh, Borjen.; Lam, Frank.; Rammer, Doug;.; Wacker, James

Publication Year: 2010  View PDF »

Category: Conference Proceedings
Associated Research Project(s):   FPL-4714-3A

Abstract: Wood structural panel sheathed shear walls and diaphragms are the primary lateral-loadresisting elements in wood-frame construction. The historical performance of light-frame structures in North America are very good due, in part, to model building codes that are designed to preserve life safety, as well as the inherent redundancy of wood-frame construction using wood structural panel shear walls and diaphragms. As wood-frame construction is continuously evolving, designers in many parts of North America are optimizing design solutions that require the understanding of force transfer between load-resisting elements.

Keywords: Buildings, testing, wooden buildings, walls, wooden-frame buildings, design, construction, structural design, structural frames, windows, doors, standards, engineering standards, shear walls, mathematical models, durability, wood construction, openings, force transfer, performance testing

Publication Review Process: Informally Refereed (Peer-Reviewed)

File size: 590 kb(s)

Date posted: 05/16/2011

This publication is also viewable on Treesearch:  view
RITS Product ID: 36154
Current FPL Scientists associated with this product (listed alphabetically)
Rammer, Douglas R.
Research General Engineer
Wacker, James P.
Research General Engineer
 

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »