Title: Measuring Wood Specific Gravity - Correctly

Source: American Journal of Botany 97(3): 519-524. 2010

Author(s)Williamson, G. Bruce; Wiemann, Michael C.

Publication Year: 2010  View PDF »

Category: Journal Articles
Associated Research Project(s):   FPL-4714-1A

Abstract: The specific gravity (SG) of wood is a measure of the amount of structural material a tree species allocates to support and strength. In recent years, wood specifi c gravity, traditionally a forester s variable, has become the domain of ecologists exploring the universality of plant functional traits and conservationists estimating global carbon stocks. While these developments have expanded our knowledge and sample of woods, the methodologies employed to measure wood SG have not received as much scrutiny as SG s ecological importance. Here, we reiterate some of the basic principles and methods for measuring the SG of wood to clarify past practices of foresters and ecologists and to identify some of the prominent errors in recent studies and their consequences. In particular, we identify errors in (1) extracting wood samples that are not representative of tree wood, (2) differentiating wood specifi c gravity from wood density, (3) drying wood samples at temperatures below 100 ° C and the resulting moisture content complications, and (4) improperly measuring wood volumes. In addition, we introduce a new experimental technique, using applied calculus, for estimating SG when the form of radial variation is known, a method that signifi cantly reduces the effort required to sample a tree s wood.

Keywords: Specific gravity; moisture; wood moisture; wood density; measurement; error analysis; mathematical statistics; temperature; drying; wood drying; volume; calculus; increment borers; moisture content; increment cores; Wiemann approximation; review article

Publication Review Process: Formally Refereed

File size: 467 kb(s)

Date posted: 01/10/2011

This publication is also viewable on Treesearch:  view
RITS Product ID: 36101
Current FPL Scientist associated with this product
Wiemann, Michael C.
Botanist
  

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »