Title: Mechanical Performance of Hemp Fiber Polypropylene Composites at Different Operating Temperatures

Source: Journal of REINFORCED PLASTICS AND COMPOSITES, Vol. 29, No.5 pp. 664-674; March 2010

Author(s)Tajvidi, Mehdi; Motie, Nazanin; Rassam, Ghonche; Falk, Robert H.; Felton, Colin

Publication Year: 2010  View PDF »

Category: Journal Articles
Associated Research Project(s):   FPL-4714-2A

Abstract: In order to quantify the effect of temperature on the mechanical properties of hemp fiber polypropylene composites, formulations containing 25% and 40% (by weight) hemp fiber were produced and tested at three representative temperatures of 256, 296, and 336 K. Flexural, tensile, and impact tests, as well as dynamic mechanical analysis, were performed and the reduction in mechanical properties were evaluated. Impact resistance was independent of temperature, whereas flexural and tensile properties were strongly affected. The highest reductions were observed in stiffness (modulus) values and flexural properties were reduced to a higher degree. The reductions in mechanical properties were well explained by a simple quadratic curve-fitting procedure applied to experimental data. Dynamic mechanical analysis revealed no change in glass transition temperature when the fiber content was increased but the composite material had better temperature resistance at higher fiber content. The results of the present study will be helpful in determining the end-use application of these composite materials.

Keywords: Hemp; polypropylene; impact testing; composite materials; mechanical properties; wood-plastic composites; temperature; testing; elasticity; modulus of elasticity; flexure; thermoplastic composites; fiber-reinforced plastics; plant fibers; influences; wood-plastic materials; tensile strength; dynamic mechanical analysis; strength; stiffness

Publication Review Process: Informally Refereed (Peer-Reviewed)

File size: 242 kb(s)

Date posted: 09/07/2010

This publication is also viewable on Treesearch:  view
RITS Product ID: 31056
Current FPL Scientist associated with this product
Falk, Robert H.
Research General Engineer
  

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »