Title: A laboratory facility for research on wind-driven rain intrusion in building envelope assemblies

Source: 2009 Wood and Fiber Product Seminar: VTT and USDA Joint Activity, September 22-23, 2009. Edited by Ali Harlin & Minna Vikman. (VTT Symposium 263) Helsinki, Finland : VTT, c2010. 176, A3 p. ISBN 978-951-38-7589-3.

Author(s)Glass, Samuel V.

Publication Year: 2010  View PDF »

Category: Journal Articles
Associated Research Project(s):   FPL-4723-1

Abstract: Moisture management is critical for durable, energy-efficient buildings. To address the need for research on wind-driven rain intrusion in wall assemblies, the U.S. Forest Products Laboratory is developing a new facility. This paper describes the underlying principle of this facility and its capabilities.

Keywords: Building materials; service life; weathering; moisture; research; buildings; testing; wood moisture; dampness in buildings; environmental engineering; humidity control; wooden buildings; airtightness; walls; rain; rainfall; accelerated life testing; exposure tests; durability; moisture content; forest products research; product testing; forest products laboratories; moisture content of wood in service; moisture control; accelerated testing; Chamber for Analytic Research on Wall Assemblies exposed to Simulated weather; CARWASh

Publication Review Process: Informally Refereed (Peer-Reviewed)

File size: 523 kb(s)

Date posted: 07/15/2010

This publication is also viewable on Treesearch:  view
RITS Product ID: 35771
Current FPL Scientist associated with this product
Glass, Samuel V.
Research Physical Scientist
  

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »