Title: Composites from wood and plastics

Source: 2009 Wood and Fiber Product Seminar: VTT and USDA Joint Activity, September 22-23, 2009. Edited by Ali Harlin & Minna Vikman. (VTT Symposium 263) Helsinki, Finland : VTT, c2010. 176, A3 p. ISBN 978-951-38-7589-3.

Author(s)Clemons, Craig

Publication Year: 2010  View PDF »

Category: Journal Articles
Associated Research Project(s):   FPL-4706-1A

Abstract: Composites made from thermoplastics and fillers or reinforcements derived from wood or other natural fibers are a dynamic research area encompassing a wide variety of composite materials. For example, as the use of biopolymers grows, wood and other natural fiber sources are being investigated as renewable sources of fillers and reinforcements to modify performance. Nanocellulose,whether cellulose nanocrystals or fibrillated cellulose, have interesting characteristics and offer new composite opportunities if efficient, economical, and scalable methods of producing both the reinforcements and the composites are developed. Experimental and analytical tools are being developed to evaluate the intrinsic material properties of the interphase or to examine the highly nonlinear behavior of large-scale, structural components, for example. This research will result in improved understanding of material behavior and identify new opportunities for composites that may be quite different from those currently produced.

Keywords: Composite materials, wood plastic composites, biocomposites, thermoplastic composites, nanocomposites, fillers, nanocrystals, biopolymers, renewable natural resources, research, sustainable forestry, wood-plastic materials, nanocellulose, utilization, forest resources, review article

Publication Review Process: Informally Refereed (Peer-Reviewed)

File size: 29 kb(s)

Date posted: 07/15/2010

This publication is also viewable on Treesearch:  view
RITS Product ID: 35765
Current FPL Scientist associated with this product
Clemons, Craig M.
Materials Research Engineer
  

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »