Title: Chemical Modification of Wood

Source: In: Handbook of wood chemistry and wood composites; CRC Press 2005

Author(s): Rowell

Publication Year: 2005  View PDF »

Category: Journal Articles

Abstract: For the most part, humans have made the most of wood while putting up with the -natural defects- that accompany it, such as dimensional instability and degradation due to weathering, fire, and decay. Wood is a hygroscopic resource designed to perform, in nature, in a wet environment. Nature is programmed to recycle wood in a timely way through biological, thermal, aqueous, photochemical, chemical, and mechanical degradations. In simple terms, nature builds wood from carbon dioxide and water and has all the tools to recycle it back to the starting chemicals. We harvest a green tree and convert it into dry products, and nature, with its arsenal of degrading reactions, starts to reclaim it at its first opportunity.

Keywords: Mechanical properties; wood biodegradation; wood deterioration; wood chemistry; chemical reactions; dimensional stability; modified wood

File size: 761 kb(s)

Date posted: 07/06/2009

This publication is also viewable on Treesearch:  view
RITS Product ID: 22502

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »