Title: Investigating the use of small-diameter softwood as guardrail posts (Dynamic Test Results)

Source: MwRSF Research Report no. TRP-03-179-07. Lincoln, NE : Midwest Roadside Safety Facility, University of Nebraska-Lincoln, 2007. 436 p.

Author(s)Hascall, Faller, Reid, Sicking, Kretschmann

Publication Year: 2007  View PDF »

Category: Journal Articles

Abstract: A modified version of the Midwest Guardrail System (MGS), utilizing small-diameter round wood posts, was developed, tested, and evaluated. Three systems were developed using different species of timber, Douglas Fir, Ponderosa Pine, and Southern Yellow Pine. A combination of Barrier VII computer simulation modeling and several series of cantilever bogie tests, conducted in both a rigid sleeve and soil, were used to determine the required diameter of post for each species in order to serve as an equivalent substitute for the standard steel post used in the barrier system. The final recommended nominal sizes were determined to be 184 mm (7 in.) for Douglas Fir, 203 mm (8 in.) for Ponderosa Pine, and 190 mm (7 in.) for Southern Pine. In addition, a grading criteria limiting knot size and ring density was established for each species. The final recommended knot sizes were limited to 51 mm (2 in.) and smaller for Douglas Fir, 102 mm (4 in.) or smaller for Ponderosa Pine, and 62 mm (2.5 in.) or smaller for Southern Yellow Pine. The minimum ring density for each post species was to exceed or equal 6 rings-per-inch for Douglas Fir, 6 rings-per-inch for Ponderosa Pine, and 4 rings-per-inch for Southern Yellow Pine. Two of the guardrail systems, one using Douglas Fir posts and another using Ponderosa Pine posts, were full-scale vehicle crash tested and reported in accordance to the Test Level 3 (TL-3) requirements specified in the National Cooperative Highway Research Program (NCHRP) Report No. 350, Recommended Procedures for the Safety Performance Evaluation of Highway Features. Testing of the third system, using Southern Pine posts, was not conducted based on the adequacy of previous testing on 184-mm (7 -in.) diameter Southern Yellow Pine posts on the standard W-beam guardrail system as well as a comparable post design strength to that of the other two species. The two full-scale crash tests showed that the modified Midwest Guardrail System functioned adequately for both wood species. Therefore, the three round wood post alternatives will serve as an acceptable substitute to the standard W152x13.4 (W6x9) steel post utilized in the MGS.

Keywords: Highway safety; wood posts; round posts; MGS; longitudinal barrier; w-beam guardrail; Douglas fir; ponderosa pine; Southern yellow pine; crash testing; roads; guard fences; wood poles; utilization; southern pines; Midwest Guardrail System; posts; small timbers; smallwood; small diameter timber; guardrails; roundwood

File size: 9,218 kb(s)

Date posted: 06/18/2009

This publication is also viewable on Treesearch:  view
RITS Product ID: 27947
Current FPL Scientist associated with this product
Kretschmann, David E.
Research General Engineer
  

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »