Title: RELATIONSHIPS BETWEEN MECHANICAL PROPERTIES, WEIGHT LOSS, AND CHEMICAL COMPOSITION OF WOOD DURING INCIPIENT BROWN-ROT DECAY

Source: Forest Prod. J. 52(7/8):34-39.

Author(s)Curling, Clausen, Winandy

Publication Year: 2002  View PDF »

Category: Journal Articles

Abstract: Incipient decay of wood by brown-rot fungi causes measurable strength losses in wood strength losses. The significant re-wood before measurable weight loss occurs. Previous studies have shown that the high duction in strength observed during in-levels of strength loss that occur duringmay he related to loss cipient decay is therefore likely to he in hemicellulose. This study investigates the effect of decay on hemicellulose composi-caused by hemicellulose decomposition. tion and the relationship of decay to the mechanical properties of the wood. An in vitro In softwoods, there are two principal test method was used to allow progressive sampling of southern pine exposed to hemicelluloses: galacto-glucomannan monocultures of brown-rot fungi. The wood was subsequently analyzed by mechanical (70% mannan), which makes up apesting and chemical analysis. The results demonstrated a ratio of strength tu weight proximately 60 percent of the total hemiloss of approximately 4: I. The chemical data indicated that early strength loss (up to cellulose content, and arabino-4-0-meth-40%) was associated with loss of arabinan and galactan components. Subsequent ylglucuronoxylan (65% xylan), which strength loss (greater than 40%) was associated with the loss of the mannan and xylan constitutes the remaining 40 percent. components. Significant loss of glucan (representing cellulose) was only detected at Thus, the amount of galactose-mannan greater than 75 percent modulus of rupture loss/

File size: 172 kb(s)

Date posted: 05/20/2009
Current FPL Scientist associated with this product
Clausen, Carol A.
Supervisory Research Microbiologist
  

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »