Title: Electrochemical impedance spectroscopy (EIS) as a tool for measuring corrosion of polymer-coated fasteners used in treated wood

Source: Forest Prod. J. 59(1/2):77-82

Author(s)Zelinka, Samuel L.; Ortiz-Candelaria, Lorraine; Stone, Donald S.; Rammer, Douglas R.

Publication Year: 2009  View PDF »

Category: Journal Articles
Associated Research Project(s):   FPL-4714-1A   FPL-4723-1

Abstract: Currently, many of the polymer-coated fasteners on the market are designed for improved corrosion performance in treated wood; yet, there is no way to evaluate their corrosion performance. In this study, a common technique for measuring the corrosion performance of polymer-coated metals, electrochemical impedance spectroscopy (EIS), was used to evaluate commercial fasteners in a water extract of treated wood. Fasteners were tested in an ‘‘out of the box'' condition as well as after being driven into the wood to simulate service conditions. The EIS spectra were fit to the traditional model for polymer-coated metals where the capacitors were replaced with constant-phase elements. A low frequency corrosion-time constant was measured for all of the fasteners in the out of the box condition, which implies that the barrier properties of the coating had failed before they were used.

Keywords: Plastic coating; coatings; deterioration; accelerated life testing; metals; testing; corrosion; anti-corrosives; fasteners; joints; wood preservatives; alkaline copper quat; electrical impedance spectroscopy; treated wood; connectors; accelerated testing; ACQ

File size: 531 kb(s)

Date posted: 04/27/2009

This publication is also viewable on Treesearch:  view
RITS Product ID: 28639
Current FPL Scientists associated with this product (listed alphabetically)
Rammer, Douglas R.
Research General Engineer
Zelinka, Samuel L.
Materials Research Engineer
 

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »