Title: Strength and stiffness assessment of standing trees using a nondestructive stress wave technique.

Source: (Research paper FPL-RP-585):9 p. : ill. ; 28 cm.

Author(s)Wang, Xiping.; Ross, Robert J.; McClellan, Michael.; Barbour, R. James.; Erickson, John R.; Forsman, John W.; McGinnis, Gary D.

Publication Year: 2000  View PDF »

Category: Research Papers

Abstract: Natureas engineering of wood through genetics, stand conditions, and environment creates wide variability in wood as a material, which in turn introduces difficulties in wood processing and utilization. Manufacturers sometimes find it difficult to consistently process wood into quality products because of its wide range of properties. The primary objective of this study was to investigate the usefulness of a stress wave technique for evaluating wood strength and stiffness of young-growth western hemlock and Sitka spruce in standing trees. A secondary objective was to determine if the effects of silvicultural practices on wood quality can be identified using this technique. Stress wave measurements were conducted on 168 young- growth western hemlock and Sitka spruce trees. After in situ measurements, a 2-ft- (0.61-m-) long bole section in the test span was taken from 56 felled trees to obtain small, clear wood specimens. Stress wave and static bending tests were then performed on these specimens to determine strength and stiffness. Results of this study indicate that in situ stress wave measurements could provide relatively accurate and reliable information that would enable nondestructive evaluation of wood properties in standing trees. The mean values of stress wave speed and dynamic modulus of elasticity for trees were in good agreement with those determined from small, clear wood specimens. Statistical regression analyses revealed strong relationships between stress wave properties of trees and static bending properties of small, clear wood specimens obtained from the trees. Regression models showed statistical significance at the 0.01 confidence level. Results of this study also demonstrate that the effect of silvicultural practices on wood properties can be identified with the stress wave properties of trees. This indicates that this nondestructive stress wave technique can be used to track property changes in trees and help determine how forests could be managed to meet desired wood and fiber qualities.

Keywords: Picea sitchensis, Tsuga heterophylla, forest trees, nondestructive testing, wood strength, strength testing, stress analysis, silvicultural systems, forestry practices, stiffness

File size: 256 kb(s)

This publication is also viewable on Treesearch:  view
RITS Product ID: 20968
Current FPL Scientists associated with this product (listed alphabetically)
Ross, Robert J.
Supervisory Research Gen. Engineer
Wang, Xiping
Research Forest Products Technologist
 

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »