Title: Relative drying times of 650 tropical woods : estimation by green moisture content, specific gravity, and green weight density

Source: Gen. Tech. Rep. FPL-GTR-71. Madison, WI: U.S. Department of Agriculture, Forest Service, Forest Products Laboratory. 27 p.

Author(s): Simpson, William T.; Sagoe, John A.

Publication Year: 1991  View PDF »

Category: General Technical Reports

Abstract: Many tropical species are underutilized because of their varied and frequently unknown drying properties. When handling a large number of species, harvesting and processing the species individually is impractical, and grouping species by similar drying properties is difficult. This report examines the relationship between green moisture content and specific gravity of tropical species, using data gathered from the world literature. The report shows how these data, converted to green weight density, can be used to estimate drying times and thus to group tropical species by similar estimated drying times.

Keywords: kiln drying, tropical hardwoods, specific gravity, density

File size: 2 kb(s)

This publication is also viewable on Treesearch:  view
RITS Product ID: 16679

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »