Title: Stress-wave velocity of wood-based panels: effect of moisture, product type, and material direction

Source: Forest products journal. Vol. 56, no. 1 (Jan. 2006): Pages 28-33

Author(s)Han, Guangping; Wu, Qinglin; Wang, Xiping

Publication Year: 2006  View PDF »

Category: Journal Articles

Abstract: The effect of moisture on longitudinal stress-wave velocity (SWV), bending stiffness. and bending strength of commercial oriented strandboard, plywood. particleboard. and southern pine lumber was evaluated. It was shown that the stress-wave verocity decreased in general with increases in panel moisture content (MC). At a given MC level. SWV varied with panel type and test directions. Regression equations relating SWV to MC and bending properties (modulus of elasticity [MOE] and modulus of rupture [MOR] were established for various products. Both MOE and MOR at different MCs can be estimated by observing the speed of propagation of a longitudinal wave. This information is useful for developing moisture correction factors on the stress-wave related properties for wood-based panel products.

Keywords: Lumber, moisture, modulus of elasticity, elasticity, wave mechanics, stress waves, bending, particle board, nondestructive testing, plywood, southern pine, oriented strandboard, OSB, stiffness, bending strength, moisture content

File size: 198 kb(s)

This publication is also viewable on Treesearch:  view
RITS Product ID: 15431
Current FPL Scientist associated with this product
Wang, Xiping
Research Forest Products Technologist
  

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »