Title: Using nano- and micro-particles of silver in lignin analysis

Source: 2006 TAPPI International Conference on Nanotechnology : April 26-28, 2006, Atlanta, Georgia. Atlanta, GA : TAPPI Press, c2006: [11] pages.

Author(s)Agarwal, Umesh P.; Reiner, Richard S.; Ralph, Sally A.

Publication Year: 2006  View PDF »

Category: Journal Articles

Abstract: Although there are numerous techniques available to study lignin in its various states, they all have limitations and to extract most amount of information, a number of analytical techniques have to be jointly used. We have recently started applying a new approach to lignin analysis - namely using nano- and micro-particles of silver for study of native and residual lignins by surface enhanced Raman spectroscopy (SERS). Silver particles were used for their unique electronic and optical properties (in this case, localized surface plasmon resonance). The SERS technique is highly sensitive and extremely selective. These attributes allow detection of small amount of lignin in presence of other constituents in a sample. For example, in wood and pulp samples, no signal from carbohydrates was detected and lignin was analyzed directly. Additionally, isolated milled- wood lignin was investigated with high sensitivity. This nano- and micro- particle based sensing could make a significant contribution to investigating lignin in difficult-to-analyze samples.

Keywords: Silver, nanotechnology, forest products industry, technological innovations, raman spectroscopy, spectrum analysis, lignin analysis, surface enhanced Raman spectroscopy, SERS

File size: 837 kb(s)

This publication is also viewable on Treesearch:  view
RITS Product ID: 11762
Current FPL Scientist associated with this product
Agarwal, Umesh P.
Research Chemist
  

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »