Title: Nondestructive assessment of timber bridges using a vibration-based method

Source: Proceedings of the 2005 structures congress, 2005 April 20-24, New York, NY. New York, NY : The Structural Engineering Institute of the American Society of Civil Engineers, 2005: [12] pages.

Author(s)Wang, Xiping; Wacker, James P.; Ross, Robert J.; Brashaw, Brian K.

Publication Year: 2005  View PDF »

Category: Journal Articles

Abstract: This paper describes an effort to develop a global dynamic testing technique for evaluating the overall stiffness of timber bridge superstructures. A forced vibration method was used to measure the natural frequency of single-span timber bridges in the laboratory and field. An analytical model based on simple beam theory was proposed to represent the relationship between the first bending mode frequency and bridge stiffness (characterized as EI product). The results indicated that the forced vibration method has potential for quickly assessing superstructure stiffness of timber bridges, but improvements must be made in measurement system to correctly identify the first bending mode frequency in bridges in the field. The beam theory model was found to fit the physics of the superstructure of single-span timber bridges and could be used to correlate first bending frequency to globalstiffness if appropriate system parameters are identified.

Keywords: Nondestructive testing, timber bridges, vibration methods, stiffness, bending

File size: 326 kb(s)

This publication is also viewable on Treesearch:  view
RITS Product ID: 16916
Current FPL Scientists associated with this product (listed alphabetically)
Ross, Robert J.
Supervisory Research Gen. Engineer
Wacker, James P.
Research General Engineer
Wang, Xiping
Research Forest Products Technologist

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »