Title: Copper tolerance of brown-rot fungi : oxalic acid production in southern pine treated with arsenic-free preservatives

Source: International biodeterioration & biodegradation. Vol. 56 (2005): Pages 75-79.

Author(s)Green, Frederick; Clausen, Carol A.

Publication Year: 2005  View PDF »

Category: Journal Articles

Abstract: The voluntary withdrawal of chromated copper arsenate (CCA)-treated wood from most residential applications has increased the use of non-arsenical copper-based organic wood preservatives. Because the arsenic component of CCA controlled copper tolerant fungi, scientists have renewed interest in and concern about the decay capacity in the important copper-tolerant group of brown-rot fungi. We have demonstrated that the primary means of inactivating copper in preservatives is by excess production of oxalic acid (OA). Oxalic acid production is a key metabolic indicator of brown- rot decay, and our objective was to estimate the production of OA in five commercial or experimental arsenic-free preservatives. Ten aggressive brown-rot fungi, chosen from previous studies and representing the genera Antrodia, Coniophora, Gloeophyllum, Postia, Serpula, Tyromyces, and Wolfiporia, were tested against southern yellow pine (SYP) blocks that were vacuum-treated with ground contact retentions of copper naphthenate, amine copper azole, alkaline copper quat type D (ACQ-D), N,N-naphthaloylhydroxylamine (NHA), and copper borate in a 12-week soil-block test. After determination of block weight loss, blocks were also tested for the presence of OA. Weight loss ranged from 0.3% to 8.3% for treated blocks and from 16.4% to 59.6% for untreated controls. We conclude that SYP treated with these five preservatives limited OA production and prevented decay, and thus confirmed the efficacy of the co-biocides against coppertolerant fungi.

Keywords: Brown-rot decay; copper-tolerant fungi; oxalic acid

File size: 70 kb(s)

This publication is also viewable on Treesearch:  view
RITS Product ID: 16808
Current FPL Scientists associated with this product (listed alphabetically)
Clausen, Carol A.
Supervisory Research Microbiologist
Green, Frederick
Research Microbiologist
 

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »