Title: PLYMAP : a computer simulation model of the rotary peeled softwood plywood manufacturing process

Source: Gen. Tech. Rep, FPL-GTR-65. Madison, WI: U.S. Department of Agriculture, Forest Service, Forest Products Laboratory. 54 p.

Author(s)Spelter, Henry

Publication Year: 1990  View PDF »

Category: General Technical Reports

Abstract: This report documents a simulation model of the plywood manufacturing process. Its purpose is to enable a user to make quick estimates of the economic impact of a particular process change within a mill. The program was designed to simulate the processing of plywood within a relatively simplified mill design. Within that limitation, however, it allows a wide range of options to be incorporated so as to customize the program to a variety of situations. The program should not be confused with a linear program-based optimization model. This program does not seek an optimum solution from a range of alternatives, but only makes calculations based upon user-entered assumptions.

Keywords: Process simulation; modeling; plywood

File size: 405 kb(s)

This publication is also viewable on Treesearch:  view
RITS Product ID: 16675
Current FPL Scientist associated with this product
Spelter, Henry N.
Economist (Volunteer)
  

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »