Title: Curbing indoor mold growth with mold inhibitors

Source: Proceedings from the Woodframe Housing Durability and Disaster Issues Conference : October 4-6, 2004 ... Las Vegas, Nevada, USA. Madison, WI : Forest Products Society, 2004: Pages 303-306.

Author(s)Clausen, Carol A.; Yang, Vina W.

Publication Year: 2004  View PDF »

Category: Journal Articles

Abstract: Environmentally acceptable mold inhibitors are needed to curb the growth of mold fungi in woodframe housing when moisture management measures fail. Excess indoor moisture can lead to rapid mold establishment which, in turn, can have deleterious affects on indoor air quality. Compounds with known mold inhibitory properties and low mammalian toxicity, such as food preservatives, pharmaceuticals, agricultural fungicides, wood preservatives, or plant extractives were evaluated individually and in combination for their ability to inhibit three common mold fungi on wood-based building materials. Dip-treatment of southern pine wood and southern pine oriented strandboard with azole-derivatives and plant extractives combined with borate-based compounds effectively prevented mold Introduction growth.

Keywords: Indoor mold; mold inhibitors; mold growth; southern pine

File size: 72 kb(s)

This publication is also viewable on Treesearch:  view
RITS Product ID: 16728
Current FPL Scientist associated with this product
Clausen, Carol A.
Supervisory Research Microbiologist
  

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »