Title: Controlling moisture content of wood samples using a modified soil-pan decay method

Source: Forest products journal. Vol. 55, no. 6 (June 2005): Pages 80-85.

Author(s)Winandy, Jerrold E.; Curling, Simon F.; Lebow, Patricia K.

Publication Year: 2005  View PDF »

Category: Journal Articles

Abstract: In wood, the threshold level below which decay cannot occur varies with species or type of wood product and other factors such as temperature, humidity, and propensity of exposure or service-use to allow rain-induced wetting and subsequent drying. The ability to control wood moisture content (MC) during laboratory decay testing could allow research on the moisture thresholds required for the initiation of wood decay over a range ofmoisture conditions. In this study, we modified the soil-pan decay test method to control wood MC by controlling the vermiculite moisture levels. A model was developed to understand and control wood MC when using this modified soil-pan decay method.

Keywords: Soil-pan decay method, moisture content, wood moisture, vermiculite

File size: 559 kb(s)

This publication is also viewable on Treesearch:  view
RITS Product ID: 15295
Current FPL Scientist associated with this product
Lebow, Patricia K.
Mathematical Statistician
  

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »