Title: Relationship between stress wave velocities of green and dry veneer

Source: Forest products journal. Vol. 54, no. 6 (June 2004): Pages 85-89

Author(s)Brashaw, Brian K.; Wang, Xiping; Ross, Robert J.; Pellerin, Roy F.

Publication Year: 2004  View PDF »

Category: Journal Articles

Abstract: This paper evaluates the relationship between the stress wave velocities of green and dry southern pine and Douglas-fir veneers. A commercial stress wave timer and a laboratory signal analysis system were used to measure the transit time required for an induced stress wave to travel the longitudinal length of each veneer. Stress wave transit times were measured in the veneers in the wet condition and at a dry equilibrated moisture content of approximately 10 percent. A strong linear relationship was found between green and dry stress wave velocity for both southern pine and Douglas-fir veneers. The strength of the relationship was improved significantly when the signal analysis system was used.

Keywords: Green veneer, dry veneer, veneer, southern pine, Douglas-fir, stress wave velocities, non-destructive testing, wood properties

File size: 59 kb(s)

This publication is also viewable on Treesearch:  view
RITS Product ID: 12569
Current FPL Scientists associated with this product (listed alphabetically)
Ross, Robert J.
Supervisory Research Gen. Engineer
Wang, Xiping
Research Forest Products Technologist
 

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »