Title: The effect on biological and moisture resistance of epichlorohydrin chemically modified wood

Source: Thirty-third annual meeting of the International Research Group on Wood Preservation, 2002 May 12-17, Cardiff, South Wales, UK. Stockholm, Sweden : IRG Secretariat, [2002]: 11 pages.

Author(s)Ibach, Rebecca E.; Lee, Beom-Goo

Publication Year: 2002  View PDF »

Category: Journal Articles

Abstract: Southern pine solid wood and fiber were chemically modified with epichlorohydrin to help in understanding the role of moisture in the mechanism of biological effectiveness of chemically modified wood. The solid wood had weight gains from 11% to 34%, while the fiber had weight gains from 9% to 75%. After modification, part of the specimens were water leached for 2 weeks or extracted for 2 hours with a toluene:ethanol (2:1) solution. The equilibrium moisture content (EMC) at 30%, 65%, and 90% relative humidity (RH) and 27 C was determined on all specimens. Laboratory soil block decay testing using the brown-rot fungus Gloeophyllum trabeum was performed and weight loss calculated. Results show that epichlorohydrin modified specimens did not lower the EMC significantly, yet there was biological effectiveness at 31% weight gain for the solid wood and 60% weight gain for the fiber. This indicates that the mechanism of efficacy may be due to substrate modification rather than moisture exclusion. Energy dispersive x-ray analysis (EDXA) was performed locating the chlorine throughout the wood cell wall.

Keywords: Chemical modification, epichlorohydrin, equilibrium moisture content, brown-rot fungus, energy dispersive x-ray analysis, solid wood, fiber

File size: 203 kb(s)

This publication is also viewable on Treesearch:  view
RITS Product ID: 12003
Current FPL Scientist associated with this product
Ibach, Rebecca E.
Research Chemist
  

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »