Title: Nondestructive evaluation of oriented strand board exposed to decay fungi.

Source: Thirty-third Annual Meeting of the International Research Group on Wood Preservation, 2002 May 12-17, Cardiff, South Wales, UK. Stockholm, Sweden : IRG Secretariat, 2002. IRG/WP ; 02-20243: [6] pages.

Author(s)Illman, Barbara L.; Yang, Vina W.; Ross, Robert J.; Nelson, William J.

Publication Year: 2002  View PDF »

Category: Journal Articles

Abstract: Stress wave nondestructive evaluation (NDE) technologies are being used in our laboratory to evaluate the performance properties of engineered wood. These techniques have proven useful in the inspection of timber structures to locate internal voids and decayed or deteriorated areas in large timbers. But no information exists concerning NDE and important properties of wood composites exposed to decay fungi. For our pilot study on several types of wood composites, we examined the relationship between nondestructive stress wave transmission, decay rate and the bending properties of OSB exposed to the brown-rot fungus, Gloeophyllum trabeum (MAD-617). The following measurements were taken: stress wave transmission time (pulse echo test method), static bending test (ASTM D3043-95), and decay (expressed as percent weight). Stress wave measurements correlated with strength loss and with increasing rate of fungal decay. Stress wave NDE has great potential as a method for inspection of wood composite load-bearing (in-service) structures, detection of decay in laboratory tests, assessment of chemical additives to improve wood composite durability, and prediction of long term composite performance.

Keywords: Decay fungi, OSB, NDE, stress wave evaluation.

File size: 471 kb(s)

This publication is also viewable on Treesearch:  view
RITS Product ID: 11827
Current FPL Scientists associated with this product (listed alphabetically)
Illman, Barbara L.
Supervisory Plant Pathologist
Ross, Robert J.
Supervisory Research Gen. Engineer
 

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »