Title: Tolerance of Serpula lacrymans to copper-based wood preservatives

Source: International biodeterioration & biodegradation. Vol 56 (2005): Pages 173-177

Author(s)Hastrup, Anne Christine Steenkjaer; Green, Frederick; Clausen, Carol A.; Jensen, Bo

Publication Year: 2005  View PDF »

Category: Journal Articles

Abstract: Serpula lacrymans, the dry rot fungus, is considered the most economically important wood decay fungus in certain temperate regions of the world, namely northern Europe, Japan, and Australia. Previously, copper-based wood preservatives were commonly used for pressure treatment of wood for building construction, but some decay fungi are known to be copper tolerant. In this study, soil-block tests were undertaken to clarify the effect of copper, copper citrate, and alkaline copper quaternary-type D (ACQ-D) on the decay capabilities of S. lacrymans compared with an alternative wood preservative not containing copper. Twelve isolates of the dry rot fungus S. lacrymans and four other brown-rot species were evaluated for weight loss on wood treated with 1.2% copper citrate, 0.5% ACQ-D, and 0.5% naphthaloylhydroxylamine (NHA). Eleven out of 12 isolatcs of S. lacrymans were shown to be tolerant towards copper citrate. The ACQ-D and NHA preservatives, on the other hand, were both effective against the dry rot isolates.

Keywords: Serpula lacrymans; dry rot; copper tolerance; copper citrate; ACQ-D; NHA; brown rot; wood preservatives; wood-decaying fungi; copper; soil block testing; metal tolerance; preservatives; copper compounds; decay fungi; ammoniacal copper quat

File size: 83 kb(s)

This publication is also viewable on Treesearch:  view
RITS Product ID: 11767
Current FPL Scientists associated with this product (listed alphabetically)
Clausen, Carol A.
Supervisory Research Microbiologist
Green, Frederick
Research Microbiologist
 

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »