Title: Acoustic evaluation of standing trees : recent research development

Source: Proceedings of the 14th International Symposium on Nondestructive Testing of Wood : May 2-4, 2005, University of Applied Sceinces, Eberswalde, Germany. Aachen, Germany : Shaker Verlag, 2005: ISBN 3832239499: pages 455-465

Author(s)Wang, Xiping; Ross, Robert J.; Carter, Peter

Publication Year: 2005  View PDF »

Category: Journal Articles

Abstract: This paper presents some research results from recent trial studies on measuring acoustic velocities on standing trees of five softwood species. The relationships between tree velocities measured by time of flight method and log velocities measured by resonance method were evaluated. Theoretical and empirical models were developed for adjusting observed tree velocity values to equivalent log velocities.

Keywords: Trees, nondestructive testing, wood, grading, mechanical properties, softwoods, wood quality, acoustic testing, standing trees, acoustic velocity

File size: 119 kb(s)

This publication is also viewable on Treesearch:  view
RITS Product ID: 11520
Current FPL Scientists associated with this product (listed alphabetically)
Ross, Robert J.
Supervisory Research Gen. Engineer
Wang, Xiping
Research Forest Products Technologist
 

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »