Title: The use of electrochemical impedance spectroscopy (EIS) to measure the corrosion of metals in contact with wood

Source: TMS letters [electronic resource]. Vol. 2, no. 1 (2005): pages 15-16.

Author(s)Zelinka, Samuel L.; Rammer, Douglas R.

Publication Year: 2005  View PDF »

Category: Journal Articles

Abstract: Although preservative treatments prolong the life of wood, they can also contribute to the corrosion of fasteners. The corrosion of fasteners merits further study because it can affect the long-term durability of structures and fundamental knowledge of corrosion in wood is limited. The goal of this study is to determine the viability of electrochemical impedance spectroscopy (EIS) as an accelerated testing procedure for determining the corrosion rate of metals in water-saturated wood.

Keywords: Accelerated life testing, fasteners, wood preservatives, preserved wood, metals, corrosion, anti-corrosives, electrochemical impedance spectroscopy, preservative treated wood, accelerated testing, treated wood, CCA, ACQ, preservatives, chromated copper arsenate, alkaline copper quat

File size: 140 kb(s)

This publication is also viewable on Treesearch:  view
RITS Product ID: 24092
Current FPL Scientists associated with this product (listed alphabetically)
Rammer, Douglas R.
Research General Engineer
Zelinka, Samuel L.
Materials Research Engineer
 

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »