Title: Are epoxy-wood bonds durable enough?

Source: Wood adhesives 2005 : November 2-4, 2005 ... San Diego, California, USA. Madison, WI : Forest Products Society, 2005: ISBN: 1892529459: pages 241-246.

Author(s)Frihart, Charles R.

Publication Year: 2005  View PDF »

Category: Journal Articles

Abstract: An important aspect of any adhesive bond is that the bond maintains its integrity during its end use. Epoxies form highly durable bonds with many substrates but are usually not considered capable of forming completely durable bonds with wood by standard accelerated tests. However, epoxies are sold for wood boat construction, and some data have indicated that epoxies can have sufficient exterior durability for general use in wood products. This conflicting information raises an important question. Are the reported discrepancies caused by changes in epoxy-wood bond formulations or in the use of different durability test methods? Examination of these data has led to an interfacial strain model which provides the most compelling explanation for the durability observations of epoxy-wood bonds. The results of bond failure analysis, coupled with the ability of epoxies to bond acetylated wood and give bond durability to wood primed with hydroxymethylated resorcinol or melamine-based primers add support to this model in explaining epoxy-wood bond durability results.

Keywords: Epoxy resins, adhesives, testing, resorcinol, adhesion, failures in wood, bonding, durability, melamine resins, resorcinol glues, bondline, bond strength, strength, melamine

File size: 550 kb(s)

This publication is also viewable on Treesearch:  view
RITS Product ID: 24686
Current FPL Scientist associated with this product
Frihart, Charles R.
Research Chemist
  

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »