Title: An experimental method to simulate incipient decay of wood basidiomycete fungi

Source: [The International Research Group on Wood Preservation. Section 2, Test Methodology and Assessment : 31st annual meeting, Kona, Hawaii, USA, 14-19 May 2000. Stockholm, Sweden : IRG Secretariat, 2000].:12 p. : ill.

Author(s)Curling, Simon.; Winandy, Jerrold E.; Clausen, Carol A.

Publication Year: 2000  View PDF »

Related Publications: view

Category: Journal Articles

Abstract: At very early stages of decay of wood by basidiomycete fungi, strength loss can be measured from wood before any measurable weight loss. Therefore, strength loss is a more efficient measure of incipient decay than weight loss. However, common standard decay tests (e.g. EN 113 or ASTM D2017) use weight loss as the measure of decay. A method was developed that allowed progressive removal of samples so that all stages of colonisation and decay could be monitored by strength testing, weight loss determination and chemical analysis. Our results indicated that substantial and rapid decay (90% strength loss and 40% weight loss after 12 weeks) of southern pine by brown rot fungi was possible using the method. Our results also demonstrate a direct relationship between strength loss and weight loss and suggest a quantitative relationship between strength loss and chemical composition (hemicellulose sugars) during incipient decay of southern pine by basidiomycete fungi.

Keywords: Basidiomycotina; Wood destroying fungi; Decay fungi. ; Methodology; Simulation models; Strength testing; Chemical composition

File size: 60 kb(s)

This publication is also viewable on Treesearch:  view
RITS Product ID: 22009
Current FPL Scientist associated with this product
Clausen, Carol A.
Supervisory Research Microbiologist
  

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »