Title: Bioprocessing preservative-treated waste wood

Source: [The International Research Group on Wood Preservation. Section 5, Environmental Aspects : 31st annual meeting, Kona, Hawaii, USA, 14-19 May 2000. Stockholm, Sweden : IRG Secretariat, 2000].:11 p. : map.

Author(s)Illman, Barbara L.; Yang, Vina W.; Ferge, Les.

Publication Year: 2000  View PDF »

Related Publications: view

Category: Journal Articles

Abstract: Disposal of preservative-treated waste wood is a growing problem worldwide. Bioprocessing the treated wood offers one approach to waste management under certain conditions. One goal is to use wood decay fungi to reduce the volume of waste with an easily managed system in a cost-effective manner. Wood decay fungi were obtained from culture collections in the Mycology Center and Biodeterioration research unit at the USDA-FS Forest Products Laboratory (FPL), Madison, Wisconsin, and from FPL field sites. The 95 isolates had originally been taken from at least 66 sites from around the United States. Isolates were screened in a bioassay (known as the *choice testa) for tolerance to CCA, ACQ, creosote and pentachlorophenol. A tolerant rating was based on fungal growth toward or on treated wood, with 17 tolerant to CCA, 21 to ACQ, 12 to creosote and 5 to pentachlorophenol. Decay capacity of the tolerant isolates was determined as percent weight loss by the ASTM D-1413-76 soil bottle method. We identified 8 isolates for experiments on preservative remediation. Isolates of Meruliporia incrassata and Antrodia radiculosa gave the highest percent degradation of ACQ and CCA-treated wood. Several A. radiculosa isolates and a Neolentinus lepideus isolate grew on creosote-treated wood, but had only a 4-5% weight loss. In this paper we discuss the potential use of decay fungi to degrade or remediate preservative-treated wood.

Keywords: Wood destroying fungi; Decay fungi; Waste wood; Wood preservatives; Waste management; Creosote; Copper chrome arsenates; Bioassays; Biodegradation; Bioprocessing; Antrodia radiculosa; Meruliporia incrassata; Neolentinus lepideus; Pentachlorophenol.

File size: 95 kb(s)

This publication is also viewable on Treesearch:  view
RITS Product ID: 21953
Current FPL Scientist associated with this product
Illman, Barbara L.
Supervisory Plant Pathologist
  

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »