Title: An inverse moisture diffusion algorithm for the determination of diffusion coefficient

Source: [Proceedings of the 12th International Drying Symposium IDS2000 : 28-31 August 2000 : Noordwijkerhout, The Netherlands. Amsterdam, The Netherlands : Elsevier, 2000].:9 p. : ill.

Author(s)Liu, Jen Y.; Simpson, William T.; Verrill, Steve P.

Publication Year: 2000  View PDF »

Category: Journal Articles

Abstract: The finite difference approximation is applied to estimate the moisture-dependent diffusion coefficient by utilizing test data of isothermal moisture desorption in northern red oak (Quercus rubra). The test data contain moisture distributions at discrete locations across the thickness of specimens, which coincides with the radial direction of northern red oak, and at specified times. Also, the rate of moisture variation at each specified time and location must be known or correctly estimated. The functional form of the diffusion coefficient as well as the boundary conditions at the surfaces are not known a priori. The resulting system of finite difference equations defines an inverse problem, whose solution may be sensitive to small changes of input data. Results indicate that the diffusion coefficient increases with increasing moisture content below the fiber saturation point, which defines the upper limit applied by the diffusion theory.

Keywords: Quercus rubra, Wood moisture, Moisture content, Diffusion, Algorithms, Equations

File size: 95 kb(s)

This publication is also viewable on Treesearch:  view
RITS Product ID: 21915
Current FPL Scientist associated with this product
Verrill, Steve P.
Mathematical Statistician
  

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »