Title: Wood Biomass for Energy

Source: USDA Forest Service, Forest Products Laboratory, Techlines, 2004

Author(s): PCAdele

Publication Year: 2004  View PDF »

Related Publications: view

Category: TechLines

Abstract: Wood fuel has several environmental advantages over fossil fuel. The main advantage is that wood is a renewable resource, offering a sustainable, dependable supply. Other advantages include the fact that the amount of carbon dioxide (CO2) emitted during the burning process is typically 90% less than when burning fossil fuel. Wood fuel contains minimal amounts of sulfur and heavy metals. It is not a threat to acid rain pollution, and particulate emissions are controllable.

Keywords: -Biomass, energy, gasification, cogeneration, combustion, cofiring, heat, power, Techline-

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »