Requested Product

Title: Defining Hardwood Veneer Log Quality Attributes

Source: Gen. Tech. Rep. NE-313. Newtown Square, PA: U.S. Department of Agriculture, Forest Service, Northeastern Research Station. 36 p.

Author(s)Wiedenbeck, Jan; Wiemann, Michael; Alderman, Delton; Baumgras, John; Luppold, William

Publication Year: 2004  View PDF »

Category: General Technical Reports

Abstract: This publication provides a broad spectrum of information on the hardwood veneer industry in North America. Veneer manufacturers and their customers impose guidelines in specifying wood quality attributes that are very discriminating but poorly defined (e.g., exceptional color, texture, and/or figure characteristics). To better understand and begin to define the most important attributes that distinguish veneer logs from sawlogs, and high-end from low-end veneer logs, we visited and interviewed veneer log buyers and sellers, veneer manufacturers, and veneer sales personnel. The first section of this report provides information on the demographics of the hardwood veneer industry and domestic and export market influences on veneer manufacturing. This is followed by a discussion of: 1) veneer quality requirements for different product markets, 2) veneer log quality evaluation procedures, 3) veneer log procurement systems, 4) regional variations in veneer log quality characteristics, and 5) species-specific quality requirements and issues.

Keywords: veneer, quality, hardwood, slicing, appearance-grade, flitch

Publication Review Process: Informally Refereed (Peer-Reviewed)

File size: 2,035 kb(s)

Date posted: 06/06/2018

This publication is also viewable on Treesearch:  view
RITS Product ID: 8418

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »