Title: Influence of a mineral insecticide particle size on bait efficacy against Reticulitermes flavipes (Isoptera: Rhinotermitidae)

Source: Sociobiology, Vol. 50(2): 521-533

Author(s)Shelton, Thomas g.; Cartier, Laurent; Wagner, Terence L.; Becker, Christian

Publication Year: 2007  View PDF »

Category: Not Classified

Abstract: We examined the efficacy of termiticidal baits comprised of powdered acellulose and a mineral insecticide, cryolite crystals, in laboratory bioassays against pseudergates of Eastern subterranean termites [Reticulitermes flavipes (Kollar)]. The influence of cryolite crystal size [0 (control), 0.2, and 20 pm diameter particles] on the overall mortality of termites consuming the bait was determined in forced feeding bioassays. Only baits containing 20 pm diameter cryolite crystals increased termite mortality significantly above the control treatment. An additional study examining feeding on stained bait (control and 20 pm diameter cryolite crystals only) indicated that termites will consume the bait, and that termite mortality from feeding on the bait increases over time.

Keywords: termite control, baits, inorganic pesticides, Reticulitermes flavipeS

File size: 1,024 kb(s)

Date posted: 04/17/2008

This publication is also viewable on Treesearch:  view
RITS Product ID: 1801
Current FPL Scientist associated with this product
Shelton, Thomas Guy
Research Entomologist
  

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »