Please wait...

Banner for LabNotes
From Lab Notes
Contact Information
Forest Products Laboratory
One Gifford Pinchot Drive
Madison, WI 53726-2398
Phone: (608) 231-9200
Fax: (608) 231-9592
Email

 

You are here: FPL Home  / Information  / Publications, Presentations & Datasets  / Publications - All Chapters

All chapters for the publication: Dry Kiln Operator's Manual - USDA Agricultural Handbook AH-188

Below are the 12 chapters for the requested publication Dry Kiln Operator's Manual - USDA Agricultural Handbook AH-188. You may re-sort the listing by: 


Publication Year: 2001
Title: Chapter 01 Properties of Wood Related to Drying
Source: USDA Agricultural Handbook AH-188: Dry Kiln Operator's Manual
Author(s) Simpson
Year: 2001   view abstract, download publication »



Title: Chapter 02 Kiln Types and Features
Source: USDA Agricultural Handbook AH-188: Dry Kiln Operator's Manual
Author(s) Boone, Simpson
Year: 2001   view abstract, download publication »



Title: Chapter 03 Dry Kiln Auxiliary Equipment
Source: USDA Agricultural Handbook AH-188: Dry Kiln Operator's Manual
Author(s) Boone
Year: 2001   view abstract, download publication »



Title: Chapter 04 Inspection and Maintenance of Dry Kilns and Equipment
Source: USDA Agricultural Handbook AH-188: Dry Kiln Operator's Manual
Author(s) Boone, Simpson
Year: 2001   view abstract, download publication »



Title: Chapter 05 Stacking and Loading Lumber for Kiln Drying
Source: USDA Agricultural Handbook AH-188: Dry Kiln Operator's Manual
Author(s) Simpson
Year: 2001   view abstract, download publication »



Title: Chapter 06 Kiln Samples
Source: USDA Agricultural Handbook AH-188: Dry Kiln Operator's Manual
Author(s) Simpson
Year: 2001   view abstract, download publication »



Title: Chapter 07 Kiln Schedules
Source: USDA Agricultural Handbook AH-188: Dry Kiln Operator's Manual
Author(s) Boone, Simpson
Year: 2001   view abstract, download publication »



Title: Chapter 08 Drying Defects
Source: USDA Agricultural Handbook AH-188: Dry Kiln Operator's Manual
Author(s) Ward, Simpson
Year: 2001   view abstract, download publication »



Title: Chapter 09 Operating a Dry Kiln
Source: USDA Agricultural Handbook AH-188: Dry Kiln Operator's Manual
Author(s) Simpson
Year: 2001   view abstract, download publication »



Title: Chapter 10 Log and Lumber Storage
Source: USDA Agricultural Handbook AH-188: Dry Kiln Operator's Manual
Author(s) Simpson, Ward
Year: 2001   view abstract, download publication »



Title: Chapter 11 Energy in Kiln Drying
Source: USDA Agricultural Handbook AH-188: Dry Kiln Operator's Manual
Author(s) Tschernitz
Year: 2001   view abstract, download publication »



Title: Dry Kiln Operator's Manual--Intro, glossary, index
Source: USDA Agricultural Handbook AH-188: Dry Kiln Operator's Manual
Author(s) Simpson, ed.
Year: 2001   view abstract, download publication »