Cross Laminated Timber Fire Testing

Live footage of fire testing on a full-scale cross laminated timber building. The tests are explained by two FPL researchers involved in the project. Testing demonstrated it is possible to build a fire resistant building using CLT.

You can read more specifics about the tests in this previous LabNotes blog post, or if you’re really into the details and data, check out the full FPL general technical repor.

For more information about FPL's current research initiatives, please refer to FPL's current Research Emphasis Areas below...