Banner for LabNotes
From Lab Notes
Contact Information
Forest Products Laboratory
One Gifford Pinchot Drive
Madison, WI 53726-2398
Phone: (608) 231-9200
Fax: (608) 231-9592
Email

 

You are here: FPL Home  / Information  / Employees Directory  / Profile

Nicole Stark
Nicole Stark

Nicole M. Stark

Engineered Composites Science
Unit: FPL-4706
Research Chemical Engineer
One Gifford Pinchot Drive
Madison, WI
United States
53726-2398

Phone: 608-231-9392
nicole.stark@usda.gov

Current Research

Dr. Nicole Stark's research focuses on the durability of wood-plastic composites from polymers and wood-derived. Nicole is interested in characterizing fundamental changes in surface chemistry and morphology that occur during weathering, and uses innovative processing techniques and treatments to improve weathering performance. Her research also includes incorporating alternative raw materials such as biopolymers, low-value woody biomass, and biorefinery residuals into high-value composites.


Research Interest

  • Composites from wood or other natural fibers and plastics
  • Coating wood composites for improved durability
  • Chemical modification and pre-treatment of wood fibers for enhanced composite durability
  • Changes in surface chemistry of wood-plastic composites during photodegradation
  • Moisture performance and fire performance of wood-plastic composites


Education

  • Michigan Technological University, Houghton, MI, Ph.D. Forest Science ,
  • University of Wisconsin, Madison, WI, M.S. Mechanical Engineering ,
  • University of Wisconsin, Madison, WI, B.S. Chemical Engineering ,

Professional Organizations

  • Forest Products Society (FPS), Board Member (2013 - Current)
  • Society of Plastics Engineers, Member (2004 - Current)

Below are the 104 US Forest Service publications sorted by year. You may re-sort the list by: Title, Date Posted, Category, Publication or Year.

Publication Year: 2019
 
Title: Functionalized Cellulose Nanocrystals: A Potential Fire Retardant for Polymer Composites
Source: Polymers. 11(8). 7 p.
Author(s) Bajwa, Dilpreet ; Rehovsky, Chad ; Shojaeiarani, Jamileh ; Stark, Nicole ; Bajwa, Sreekala ; Dietenberger, Mark A.
Year: 2019   view abstract, download publication »
Title: Rheological properties of cellulose nanocrystals engineered polylactic acid nanocomposites
Source: Composites Part B: Engineering. 161: 483-489.
Author(s) Shojaeiarani, Jamileh ; Bajwa, Dilpreet S.; Stark, Nicole M.; Bajwa, Sreekala G.
Year: 2019   view abstract, download publication »
Title: Wet compounding of cellulose nanocrystals into polylactic acid for packaging applications
Source: ANTEC 2019 - the plastics conference. 5 p.
Author(s) Sabo, Ronald C.; Stark, Nicole M.; Wei, Liqing ; Matuana, Laurent M.
Year: 2019   view abstract, download publication »
Publication Year: 2018
 
Title: Colemanite: a fire retardant candidate for wood plastic composites
Source: BioResources. 13(1): 1491-1509.
Author(s) Terzi, Evren; Kartal, Saip Nami; Piskin, Sabriye; Stark, Nicole; Figen, Aysel Kanturk; White, Robert H.
Year: 2018   view abstract, download publication »
Title: Effect of freeze-drying on the morphology of dried cellulose nanocrystals (CNCs) and tensile properties of poly(lactic) acid-CNC composites
Source: In: Proceedings, ANTEC®2018-society of plastics engineers. 5p.
Author(s) Stark, Nicole M.; Wei, Liquing ; Sabo, Ronald C.; Reiner, Richard R.; Matuana, Laurent M.
Year: 2018   view abstract, download publication »
Title: Green esterification: a new approach to improve thermal and mechanical properties of poly(lactic acid) composites reinforced by cellulose nanocrystals
Source: Journal of Applied Polymer Science. 135(27). 8 p.
Author(s) Shojaeiarani, Jamileh ; Bajwa, Dilpreet S.; Stark, Nicole M.
Year: 2018   view abstract, download publication »
Title: Moisture and oxygen barrier properties of cellulose nanomaterial-based films
Source: ACS Sustainable Chemistry & Engineering. 6(1): 49-70.
Author(s) Wang, Jinwu ; Gardner, Douglas J.; Stark, Nicole M.; Bousfield, Douglas W.; Tajvidi, Mehdi ; Cai, Zhiyong
Year: 2018   view abstract, download publication »
Title: Performance of high lignin content cellulose nanocrystals in poly(lactic acid)
Source: Polymer. 135: 305-313.
Author(s) Wei, Liqing; Agarwal, Umesh P.; Matuana, Laurent; Sabo, Ronald C.; Stark, Nicole M.
Year: 2018   view abstract, download publication »
Title: Spin-coating: a new approach for improving dispersion of cellulose nanocrystals and mechanical properties of poly (lactic acid) composites
Source: Carbohydrate Polymers. 190: 139-147.
Author(s) Shojaeiarani, Jamileh ; Bajwa, Dilpreet S.; Stark, Nicole M.
Year: 2018   view abstract, download publication »
Title: Water based esterification of cellulose nanofibrils for compounding with PLA
Source: In: Proceedings, forest products society 72nd international convention. 1-7.
Author(s) Lafia-Araga, Ruth A.; Sabo, Ronald C.; Stark, Nicole M.; Matuana, Laurent M.
Year: 2018   view abstract, download publication »
Title: Water vapor and oxygen barrier properties of extrusion-blown poly(lactic acid)/cellulose nanocrystals nanocomposite films
Source: Composites Part A: Applied Science and Manufacturing. 114: 204-211.
Author(s) Karkhanis, Sonal S.; Stark, Nicole M.; Sabo, Ronald C.; Matuana, Laurent M.
Year: 2018   view abstract, download publication »
Publication Year: 2017
 
Title: Blown film extrusion of poly(lactic acid) without melt strength enhancers
Source: Journal of Applied Polymer Science. 134(34): 45212-45222.
Author(s) Karkhanis, Sonal S.; Stark, Nicole M.; Sabo, Ronald C.; Matuana, Laurent M.
Year: 2017   view abstract, download publication »
Title: Chemical modification of nanocellulose with canola oil fatty acid methyl ester
Source: Carbohydrate Polymers. 169(2017): 108-116
Author(s) Wei, Liqing; Agarwal, Umesh P.; Hirth, Kolby C.; Matuana, Laurent M.; Sabo, Ronald C.; Stark, Nicole M.
Year: 2017   view abstract, download publication »
Title: Effect of compounding approaches on fiber dispersion and performance of poly(lactic acid)/cellulose nanocrystal composite blown films
Source: In: Society of Plastic Engineers, ISBN: 978-0-692-88309-9: Paper prepared for: ANTEC® 2017. Anaheim, CA. 6 p.
Author(s) Karkhanis, Sonal S.; Matuana, Laurent M.; Stark, Nicole M.; Sabo, Ronald C.
Year: 2017   view abstract, download publication »
Title: Flammability properties and radiant fraction of FRT wood plastic composites using mass loss calorimeter under HRR hood
Source: In: Proceedings, fire and materials 2017 conference. San Francisco, CA: 988-989.
Author(s) Dietenberger, Mark A.; Boardman, Charles R.; Stark, Nicole
Year: 2017   view abstract, download publication »
Title: Nanocomposites from lignin-containing cellulose nanocrystals and poly(lactic acid)
Source: In: Society of Plastic Engineers, ISBN: 978-0-692-88309-9: Paper prepared for: ANTEC® 2017. Anaheim, CA. 5 p.
Author(s) Wei, Liqing; Agarwal, Umesh; Stark, Nicole; Sabo, Ronald
Year: 2017   view abstract, download publication »
Title: Performance of poly(lactic acid)/ cellulose nanocrystal composite blown films processed by two different compounding approaches
Source: Polymer Engineering & Science. 58(11): 1965-1974.
Author(s) Karkhanis, Sonal S.; Stark, Nicole M.; Sabo, Ronald C.; Matuana, Laurent M.
Year: 2017   view abstract, download publication »
Title: Preparation and characterization of the nanocomposites from chemically modified nanocellulose and poly(lactic acid)
Source: Journal of Renewable Materials. 5(5): 410-422.
Author(s) Wei, Liqing; Luo, Shupin; McDonald, Armando G.; Agarwal, Umesh P.; Hirth, Kolby C.; Matuana, Laurent M.; Sabo, Ronald C.; Stark, Nicole M.
Year: 2017   view abstract, download publication »
Publication Year: 2016
 
Title: Cellulose nanocrystals as barrier performance enhancer of extrusion-blown PLA films for food applications
Source: In: proceedings, TechConnect
Author(s) Matuana, L. M.; Karkhanis, S. S.; Stark, Nicole; Sabo, Ronald
Year: 2016   view abstract, download publication »
Title: Modification of cellulose nanocrystals (CNCs) for use in poly(lactic acid) (PLA)-CNC composite packaging products
Source: In: Proceedings, Forest Products Society International Convention, June 28-29, 2016, Portland, OR.
Author(s) Wei, Liqing; Stark, Nicole M.; Sabo, Ronald C.; Matuana, Laurent
Year: 2016   view abstract, download publication »
Title: Opportunities for cellulose nanomaterials in packaging films: a review and future trends
Source: J. Renew. Mater. 4(5): 313-326
Author(s) Stark, Nicole M.
Year: 2016   view abstract, download publication »
Title: Techniques for characterizing lignin
Source: Lignin in Polymer Composites
Author(s) Stark, Nicole M.; Yelle, Daniel J.; Agarwal, Umesh P.
Year: 2016   view abstract, download publication »
Title: Weathering characteristics of wood plastic composites reinforced with extracted or delignified wood flour
Source: Materials 2016, 9(610).
Author(s) Chen, Yao; Stark, Nicole M.; Tshabalala, Mandla A.; Gao, Jianmin; Fan, Yongming
Year: 2016   view abstract, download publication »
Publication Year: 2015
 
Title: Chapter 20: The use of wood fibers as reinforcements in composites
Source: In: Biofiber Reinforcement in composite materials, Chapter 20; 2015; pp. 648-688.
Author(s) Matuana, L.M.; Stark, N.M.
Year: 2015   view abstract, download publication »
Title: Formation of Irreversible H-bonds in Cellulose Materials
Source: Proceedings of the 18th ISWFPC (International Symposium on Wood, Fiber, and Pulping Chemistry) held in Vienna (Sept 9 -11, 2015). 2015; pp. 18-21.
Author(s) Agarwal, Umesh P.; Ralph, Sally A.; Reiner, Rick S.; Stark, Nicole M.
Year: 2015   view abstract, download publication »
Title: Grafting of Bacterial Polyhydroxybutyrate (PHB) onto Cellulose via In Situ Reactive Extrusion with Dicumyl Peroxide
Source: Biomacromolecules
Author(s) Wei, Liqing; McDonald, Armando G.; Stark, Nicole M.
Year: 2015   view abstract, download publication »
Title: Interfacial improvements in biocomposites based on poly(3-hydroxybutyrate) and poly(3-hydroxybutyrate-co-3-hydroxyvalerate) bioplastics reinforced and grafted with α-cellulose fibers
Source: Green Chemistry, Vol. 17(10)
Author(s) Wei, Liqing; Stark, Nicole M.; McDonald, Armando G.
Year: 2015   view abstract, download publication »
Publication Year: 2014
 
Title: Chemical Modification of Kraft Lignin: Effect on Chemical and Thermal Properties
Source: BioResources, Volume 9, Number 3, 2047; pp. 5488-5500.
Author(s) Chen, Yao; Stark, Nicole M.; Cai, Zhiyong; Frihart, Charles R.; Lorenz, Linda F.; Ibach, Rebecca E.
Year: 2014   view abstract, download publication »
Title: Color and Surface Chemistry Changes of Pine Wood Flour after Extraction and Delignification
Source: BioResources, Volume 9, Number 2, 2014; pp. 2937-2948.
Author(s) Chen, Yao; Tshabalala, Mandla A.; Gao, Jianmin; Stark, Nicole M.; Fan, Yongming
Year: 2014   view abstract, download publication »
Title: Decay resistance of wood-plastic composites reinforced with extracted or delignified wood flour
Source: IRG/WP 14-40655, THE INTERNATIONAL RESEARCH GROUP ON WOOD PROTECTION Section 4, Processes and properties, Paper prepared for the 45th IRG Annual Meeting St George, Utah, USA, 11-15 May, 2014 pp. 2-9.
Author(s) Ibach, Rebecca E.; Chen, Yao; Stark, Nicole M.; Tshabalala, Mandla A.; Fan, Yongming; Gao, Jianmin
Year: 2014   view abstract, download publication »
Title: Dimensional stability of wood-plastic composites reinforced with potassium methyl siliconate modified fiber and sawdust made from beetle-killed trees
Source: Eur. J. Wood Prod. Volume 72, 2014; pp. 165–176.
Author(s) Piao, Cheng; Cai, Zhiyong; Stark, Nicole M.; Montezun, Charles J.
Year: 2014   view abstract, download publication »
Title: Laboratory investigation of fire protection coatings for creosote-treated timber railroad bridges
Source: The International Research Group on Wood Protection, Section 3, Wood Protecting Chemicals, pp. 2-15; IRG/WP 14-30639; 2014.
Author(s) Clausen, Carol A.; White, Robert H.; Wacker, James P.; Lebow, Stan T.; Dietenberger, Mark A.; Zelinka, Samuel L.; Stark, Nicole M.
Year: 2014   view abstract, download publication »
Title: Moisture Performance of wood-plastic composites reinforced with extracted and delignified wood flour
Source: In: the ANTEC 2014, The Plastics Conference, April 28-30, 2014 Rio All-Suite Holtel & Casino, Las Vegas, Nevada; SPE ANTEC 2014 pp. 2049-2053.
Author(s) Chen, Yao; Stark, Nicole M.; Tshabalala, Mandla A.; Gao, Jianmin; Fan, Yongming
Year: 2014   view abstract, download publication »
Title: Properties of wood-plastic composites (WPCs) reinforced with extracted and delignified wood flour
Source: Holzforschung 2014; 8 p.
Author(s) Chen, Yao; Stark, Nicole M.; Tshabalala, Mandla A.; Gao, Jianmin; Fan, Yongming
Year: 2014   view abstract, download publication »
Title: Thermal behavior of extracted and delignified pine wood flour
Source: Thermochimica Acta Volume 591, 2014; pp. 40–44.
Author(s) Chen, Yao; Tshabalala, Mandla A.; Gao, Jianmin; Stark, Nicole M.; Fan, Yongming; Ibach, Rebecca E.
Year: 2014   view abstract, download publication »
Publication Year: 2013
 
Title: Chapter 6: New Products and Product Categories in the Global Forest Sector
Source: In Hansen , E.; Panwar , R.; Vlosky, R., Eds. CRC Press: Boca Raton, 2013; pp 129-149.
Author(s) Cai, Zhiyong; Rudie, Alan W.; Stark, Nicole M.; Sabo, Ronald C.; Ralph, Sally A.
Year: 2013   view abstract, download publication »
Title: Color and surface chemistry changes of extracted wood flour after heating at 120 °C
Source: Wood Sci Technol Volume, 48 2014; pp. 137-150.
Author(s) Chen, Yao; Tshabalala, Mandla A.; Gao, Jianmin; Stark, Nicole M.
Year: 2013   view abstract, download publication »
Title: Effect of environmental conditions on the mechanical properties and fungal degradation of polycaprolactone/microcrystalline cellulose/wood flour composites
Source: BioResources Volume 8, Number 3, pp.3322-3335; 2013
Author(s) Sabo, Ronald; Jin, Liwei; Stark, Nicole; Ibach, Rebecca E.
Year: 2013   view abstract, download publication »
Title: Influence of a stabilized cap layer on the photodegradation of coextruded high density polyethylene/woodflour composites
Source: Journal of Vinyl & Additive Technology. 239-249.
Author(s) Jin, Shan; Stark, Nicole M.; Matuana, Laurent M.
Year: 2013   view abstract, download publication »
Title: Lignin-based Phenol-Formaldehyde Resins from Purified CO2 Precipitated Kraft lignin (PCO2KL)
Source: In: International Conference on Wood Adhesives, October 9-11, 2013 Toronto, Ontario Canada from CD ISBN: 978-0-935018-37-0; 2013; pp. 601-610.
Author(s) Chen, Yao; Frihart, Charles R.; Cai, Zhiyong; Lorenz, Linda F.; Stark, Nicole M.
Year: 2013   view abstract, download publication »
Title: Lignin-based Phenol-Formalehyde Resins from Purified CO2 Precipitated Kraft Lignin (PCO2KL)
Source: In: International Conference on Wood Adhesives, 2013; pp. 601-610.
Author(s) Chen, Yao; Frihart, Charles R.; Cai, Zhiyong; Lorenz, Linda F.; Stark, Nicole M.
Year: 2013   view abstract, download publication »
Title: Potassium methyl siliconate-treated pulp fibers and their effects on wood plastic composites: Water sorption and dimensional stability
Source: Journal of Applied Polymer Science, Volume 129, Number 1, 2013; pp. 193-201.
Author(s) Piao, Cheng; Cai, Zhiyong; Stark, Nicole M.; Monlezun, Charles J.
Year: 2013   view abstract, download publication »
Title: Thermal Properties of Extracted and Delignified Wood Flour for use in Wood-Plastic Composites
Source: In: Conference Proceedings, The Advancements in Fiber-Polymer Composites: Wood Fiber, Natural Fibers and Nanocellulose, May 6-7, 2013 Milwaukee, Wisconsin. 10 p.
Author(s) Chen, Yao; Tshabalala, Mandla A.; Stark, Nicole M.; Gao, Jianmin; Fan, Yongming; Ibach, Rebecca E.
Year: 2013   view abstract, download publication »
Publication Year: 2012
 
Title: Chemical Modification of Soy Flour Protein and its Properties
Source: Advanced Materials Research Vols. 343-344 (2012) pp 875-881; 2012
Author(s) Xu, Yuzhi; Wang, Chunpeng; Chu, Fuxiang; Frihart, Charles R.; Lorenz, Linda F.; Stark, Nicole M.
Year: 2012   view abstract, download publication »
Title: Heat-induced chemical and color changes of extractive-free Black Locust (Rosinia Pseudoacacia) wood
Source: BioResources Volume 7, Number 2, 2236-2248; 2012
Author(s) Chen, Yao; Gao, Jianmin; Fan, Yongming; Tshabalala, Mandla A.; Stark, Nicole M.
Year: 2012   view abstract, download publication »
Title: Miscibility and thermal behavior of poly (ε-caprolactone)/long-chain ester of cellulose blends
Source: Carbohydrate Polymers, 88 (2012) 422-427
Author(s) Xu, Yuzhi; Wang, Chunpeng; Stark, Nicole M.; Cai, Zhiyong; Chu, Fuxiang
Year: 2012   view abstract, download publication »
Title: Optical property analysis of thermally and photolytically aged Eucalyptus Camaldulensis chemithermomechanical pulp (CTMP)
Source: BioResources 7(2), 1474-1487; 2012.
Author(s) Chen, Yao; Fan, Yongming; Tshabalala, Mandla A.; Stark, Nicole M.; Gao, Jianmin
Year: 2012   view abstract, download publication »
Title: Spectroscopic analysis of the role of extractives on heat-induced discoloration of black locust (Robinia pseudoacacia)
Source: Wood Material Science & Engineering 0.0:1-8; 2012.
Author(s) Chen, Yao; Fan, Yongming; Gao, Jianmin; Tshabalala, Mandla A.; Stark, Nicole M.
Year: 2012   view abstract, download publication »
Title: The Effect of Heat Treatment on the chemical and color change of Black Locust (Robinia Pseudoacacia) wood flour
Source: BioResources Volume 7, Number 1, 1157-1170, 2012.
Author(s) Chen, Yao; Fan, Yongming; Gao, Jianmin; Stark, Nicole M.
Year: 2012   view abstract, download publication »
Publication Year: 2011
 
Title: Fire performance testing of WPCs at the Forest Products Laboratory
Source: Proceedings of the 5th International Wood Fibre Polymer Composites Symposium : natural fibre to building and furniture products: contributing to the green growth, 2011 September 26-27, Biarritz, France. Paris, France : FCBA Institut Technologique, 2011: [11] p.
Author(s) Stark, Nicole M.; White, Robert H.
Year: 2011   view abstract, download publication »
Title: Recent activities in flame retardancy of wood-plastic composites at the Forest Products Laboratory
Source: In: 22nd annual conference on Recent Advances in Flame Retardancy of Polymeric Materials, May 23-25, 2011, Stamford Marriott Hotel and Spa, stamford, CT, ISBN 1-59623-619-1; 2011
Author(s) White, Robert H.; Stark, Nicole M.; Ayrilmis, Nadir
Year: 2011   view abstract, download publication »
Title: Ultraviolet weathering of HDPE/wood-flour composites coextruded with a clear HDPE cap layer
Source: Polymer Degradation and Stability, 96 (2011) 97-106. doi:10.1016/j.polymdegradstab.2010.10.003; 2011
Author(s) Matuana, Laurent M.; Jin, Shan; Stark, Nicole M.
Year: 2011   view abstract, download publication »
Title: Ultraviolet weathering of WPCs coextruded with a clear cap layer
Source: Proceedings of the 5th International Wood Fibre Polymer Composites Symposium : natural fibre to building and furniture products: contributing to the green growth, 2011 September 26-27, Biarritz, France. Paris, France : FCBA Institut Technologique, 2011: 12 p.
Author(s) Matuana, Laurent M.; Stark, Nicole M.; Jin, Shan
Year: 2011   view abstract, download publication »
Publication Year: 2010
 
Title: .Wood Handbook, Wood as an Engineering Material (All Chapters)
Source: Forest Products Laboratory. Wood handbook - Wood as an engineering material. General Technical Report FPL-GTR-190. Madison, WI: U.S. Department of Agriculture, Forest Service, Forest Products Laboratory: 508 p. 2010
Author(s) Bergman, Richard; Cai, Zhiyong; Carll, Charlie G.; Clausen, Carol A.; Dietenberger, Mark A.; Falk, Robert H.; Frihart, Charles R.; Glass, Samuel V.; Hunt, Christopher G.; Ibach, Rebecca E.; Kretschmann, David E.; Rammer, Douglas R.; Ross, Robert J.; Star
Year: 2010   view abstract, download publication »
Title: Durability of Wood-Plastic Composites
Source: Tenth International Conference on Wood & Biofiber Plastic Composites and Cellulose Nanocomposites Sysmposium, May 11-13, Madison, WI. Madison, WI : Forest Products Society, c2010. ISBN 978-1-892529-55-8. pp. 71-75; 2010
Author(s) Morrell, J.J.; Stark, Nicole M.; Pendleton, David E.; McDonald, Armando G.
Year: 2010   view abstract, download publication »
Title: Effect of Fire Retardants on Heat Release Rate of Wood Flour-Polyethylene Composites
Source: Tenth International Conference on Wood & Biofiber Plastic Composites and Cellulose Nanocomposites Sysmposium, May 11-13, Madison, WI. Madison, WI : Forest Products Society, c2010. ISBN 978-1-892529-55-8. pp. 103-109; 2010
Author(s) Stark, Nicole M.; Mueller, Scott A.; White, Robert H.; Osswald, Tim A.
Year: 2010   view abstract, download publication »
Title: Evaluation of various fire retardants for use in wood flour-polyethylene composites
Source: Polymer Degradation and Stability, 95 (2010) 1903-1910. doi:10.1016/j.polymdegradstab.2010.04.014; 2010
Author(s) Stark,Nicole M.; White, Robert H.; Mueller, Scott A.; Osswald, Tim A.
Year: 2010   view abstract, download publication »
Title: Wood Handbook, Chapter 11: Wood-Based Composite Materials-Panel Products- Glued-Laminated Timber, Structural Composite Lumber, and Wood-Nonwood Composite Materials
Source: General Technical Report FPL-GTR-190. Madison, WI: U.S. Department of Agriculture, Forest Service, Forest Products Laboratory: 11-1 - 11-28. Chapter 11.
Author(s) Stark, Nicole M.; Cai, Zhiyong; Carll, Charlie G. ;
Year: 2010   view abstract, download publication »
Publication Year: 2009
 
Title: Co-Extrusion of WPCs with a Clear Cap Layer to Improve
Source: In Proceedings: 4th Wood Fibre Polymer Composites International Symposium: March 30-31, 2009, Bordeaux, France; pp 1-13; 2009
Author(s) Stark, Nicole M.; Matuana, Laurent M.
Year: 2009   view abstract, download publication »
Title: FEASIBILITY OF USING SALTCEDAR AS A FILLER IN INJECTION-MOLDED POLYETHYLENE COMPOSITES
Source: Wood and Fiber Science, 41(1), 2009, pp. 2 - 12 ; 2009
Author(s) Clemons, Stark
Year: 2009   view abstract, download publication »
Publication Year: 2008
 
Title: Improving the color stability of wood-plastic composites through fiber pre-treatment
Source: Wood and fiber science. Vol. 40, no. 2 (2008): Pages 271-278
Author(s) Stark, Nicole M.; Mueller, Scott A.
Year: 2008   view abstract, download publication »
Title: Outdoor durability of wood-polymer composites; chapter 7
Source: In: Wood-polymer Composites, CRC Press, Boca Raton, Boston, New York, Washington, DC; pp. 142-165; 2008
Author(s) Stark, Gardner
Year: 2008   view abstract, download publication »
Title: Wood-plastic composites using thermomechanical pulp made from oxalic acid-pretreated red pine chips
Source: Global WPC and Natural Fibre Composites Congress and Exhibition : June 18-19, 2008, Kassel, Institut fur Werkstofftechnik, Kunststoff-und Recyclingtechnik : scientific presentations. Szczecin, Poland : PPH ZAPOL Dmochowski, Sobczyk Spolka Jauna, 2008: Pag
Author(s) Winandy, J.E.; Stark, N.M.; Horn, E.
Year: 2008   view abstract, download publication »
Publication Year: 2007
 
Title: Characterization of weathered wood-plastic composite surfaces using FTIR spectroscopy, contact angle, and XPS
Source: Polymer degradation and stability. Vol. 92 (2007): pages 1883-1890.
Author(s) Stark, Nicole M.; Matuana, Laurent M.
Year: 2007   view abstract, download publication »
Title: Coating WPC's using co-extrusion to improve durability
Source: Proceedings : Coating Wood and Wood Composites : Designing for Durability, July 23-25, 2007, Seattle, WA. [S.l. : s.n.], 2007: Pages 1-12
Author(s) Stark, Nicole M.; Matuana, Laurent M.
Year: 2007   view abstract, download publication »
Title: Cone calorimeter tests of wood-based decking materials
Source: Proceedings of the 18th annual conference on recent advances in flame retardancy of polymeric materials. Norwalk, CT : BCC Research, c2007: ISBN: 1596232218: 9781596232211: Pages 326-337.
Author(s) White, Robert H.; Dietenberger, Mark A.; Stark, Nicole M.
Year: 2007   view abstract, download publication »
Title: Considerations in the weathering of wood-plastic composites
Source: Proceedings : 3rd Wood Fibre Polymer Composites International Symposium : Innovative Sustainable Materials Applied to Building and Furniture : March 26-27, 2007 ... Bordeaux, France. [S.l. : s.n.], 2007: 10 pages.
Author(s) Stark, Nicole M.
Year: 2007   view abstract, download publication »
Title: Durability and mechanical properties of silane cross-linked wood thermoplastic composites
Source: Composites science and technology. Vol. 67 (2007): pages 2728-2738.
Author(s) Bengtsson, Magnus; Stark, Nicole M.; Oksman, Kristiina
Year: 2007   view abstract, download publication »
Title: Surface characterization of weathered wood-plastic composites produced from modified wood flour
Source: 9th International Conference on Wood & Biofiber Plastic Composites : May 21-23, 2007 ... Madison, Wisconsin, USA. Madison, Wis. : Forest Products Society, 2007: Pages 271-275
Author(s) Fabiyi, James S.; McDonald, Armando G.; Stark, Nicole M.
Year: 2007   view abstract, download publication »
Title: Use of saltcedar and Utah juniper as fillers in wood-plastic composites
Source: Research Paper FPL-RP-641. Madison, WI: U.S. Department of Agriculture, Forest Service, Forest Products Laboratory. 17 pages
Author(s) Clemons, Craig; Stark, Nicole
Year: 2007   view abstract, download publication »
Publication Year: 2006
 
Title: Durability of wood-plastic composites
Source: Wood design focus. Vol. 16, no. 3 (fall 2006): pages 7-10.
Author(s) Morrell, J.J.; Stark, Nicole M.; Pendleton, David E.; McDonald, Armando G.
Year: 2006   view abstract, download publication »
Title: Effect of weathering cycle and manufacturing method on performance of wood flour and high-density polyethylene composites
Source: Journal of applied polymer science. Vol. 100 (2006): Pages 3131-3140
Author(s) Stark, Nicole M.
Year: 2006   view abstract, download publication »
Title: Influence of photostabilizers on wood flour-HDPE composites exposed to xenon-arc radiation with and without water spray
Source: Polymer degradation and stability. Vol. 91 (2006): pages 3048-3056.
Author(s) Stark, Nicole M.; Matuana, Laurent M.
Year: 2006   view abstract, download publication »
Title: Profile extrusion and mechanical properties of crosslinked wood-thermoplastic composites
Source: Polymer composites--2006. [New York] : Wiley-Interscience, 2006: pages [184]-194
Author(s) Bengtsson, Magnus; Oksman, Kristiina; Stark Nicole M.
Year: 2006   view abstract, download publication »
Publication Year: 2005
 
Title: Changes in wood flour/HDPE composites after accelerated weathering with and without water spray
Source: Proceedings of the 2nd Wood Fibre Polymer Composites Symposium : Applications and Perspectives : March 24-25, 2005, Bordeaux, France. [S.l. : s.n., 2005]
Author(s) Stark, Nicole M.
Year: 2005   view abstract, download publication »
Title: Chemistry of Wood-Plastic Composites Weathering
Source: FPL RIP-4706-003
Author(s) Dr. Armando McDonald; Dr. Nicole Stark; Dr. Mike Wolcott
Year: 2005   view abstract, download publication »
Title: Development of Wood-Plastic Composite Lumber for Low-Temperature Exterior Applications
Source: FPL RIP-4706-001
Author(s) Nicole Stark
Year: 2005   view abstract, download publication »
Title: Effect of weathering variables on the lightness of high-density polyethylene woodflour composites
Source: 8th International Conference on Wood-fiber-Plastic Composites (and other natural fibers) : May 23-25, 2005 ... Madison, Wisconsin, USA. Madison, WI : Forest Products Society: pages 207-212.
Author(s) Stark, Nicole M.
Year: 2005   view abstract, download publication »
Title: Effect of Weathering Variables on the Lightness of High-Density Polyethylene Woodflour Composites
Source: Eighth International Conference on Woodfiber-Plastic Composites, May 23-25, 2005 Monona Terrace Community & Convention Center Madison, Wisconsin, USA
Author(s) Stark
Year: 2005   view abstract, download publication »
Title: Evaluation and process development of salt cedar and juniper biocomposites as tools to utilize exotic and invasive species and restore native ecosystems
Source: 3rd International Workshop on Green Composites, Japanese Society of Material Science, Doshisha University, Kyoto, Japan, March 16-17, 2005. [S.l.] : The Society, 2005. Pages 56-60.
Author(s) Winandy, Jerrold E.; Clemons, Craig M.; Stark, Nicole M.; Muehl, James H.; Williams, R. Sam
Year: 2005   view abstract, download publication »
Title: Outdoor durability of wood-plastic composite lumber
Source: USDA Forest Service, Forest Products Laboratory, Techlines, 2005
Author(s) Stark, Nicole
Year: 2005   view abstract, download publication »
Title: Use of Exotic-Invasive Species in Wood-Plastic Composite Profiles
Source: FPL RIP-4706-002
Author(s) Nicole Stark; Craig Clemons
Year: 2005   view abstract, download publication »
Publication Year: 2004
 
Title: Considerations in recycling of wood-plastic composites
Source: 5th Global Wood and Natural Fibre Composites Symposium, April 27-28, 2004, in Kassel, Germany: [9] Pages.
Author(s) Winandy, J.E.; Stark, N.M.; Clemons, C.M.
Year: 2004   view abstract, download publication »
Title: Effect of processing method on surface and weathering characteristics of wood-flour/HDPE composites
Source: Journal of applied polymer science. Vol. 93 (2004): Pages 1021-1030
Author(s) Stark, Nicole M.; Matuana, Laurent M.; Clemons, Craig M.
Year: 2004   view abstract, download publication »
Title: Surface chemistry and mechanical property changes of wood-flour/high-density-polyethylene composites after accelerated weathering
Source: Journal of applied polymer science. Vol. 94 (2004): pages 2263-2273.
Author(s) Stark, Nicole M.; Matuana, Laurent M.
Year: 2004   view abstract, download publication »
Title: Surface chemistry changes of weathered HDPE/wood-flour composites studied by XPS and FTIR spectroscopy
Source: Polymer degradation and stability. Vol. 86 (2004): Pages 1-9
Author(s) Stark, Nicole M.; Matuana, Laurent M.
Year: 2004   view abstract, download publication »
Publication Year: 2003
 
Title: Combined ultraviolet and water exposure as a preconditioning method in laboratory fungal durability testing
Source: Seventh International Conference on Woodfiber-Plastic Composites (and other natural fibers), May 19-20, 2003 ... Madison, Wisconsin, USA. Madison, WI : Forest Products Society, 2003: Pages 61-67
Author(s) Ibach, Rebecca E.; Clemons, Craig M.; Stark, Nicole M.
Year: 2003   view abstract, download publication »
Title: Effect of processing method on accelerated weathering of wood-flour/HDPE composites
Source: Seventh International Conference on Woodfiber-Plastic Composites (and other natural fibers), May 19-20, 2003 ... Madison, Wisconsin, USA. Madison, WI : Forest Products Society, 2003: Pages 79-87
Author(s) Stark, Nicole M.; Matuana, Laurent M.; Clemons, Craig M.
Year: 2003   view abstract, download publication »
Title: Effects of wood fiber characteristics on mechanical properties of wood/polypropylene composites
Source: Wood and fiber science. Vol. 35, no. 2 (2003): Pages 167-174
Author(s) Stark, Nicole M.; Rowlands, Robert E.
Year: 2003   view abstract, download publication »
Title: Ultraviolet weathering of photostabilized wood-flour-filled high-density polyethylene composites
Source: Journal of applied polymer science. Vol. 90 (2003): Pages 2609-2617
Author(s) Stark, Nicole M.; Matuana, Laurent M.
Year: 2003   view abstract, download publication »
Publication Year: 2002
 
Title: Photostabilization of wood flour filled HDPE composites
Source: ANTEC 2002 Annual Tecnical Conference : May 5-9, 2002, San Francisco, CA. : conference proceedings. Volume II, Materials. S.l. : Society of Plastics Engineers, 2002: p. 2209-2213
Author(s) Stark, Nicole M.; Matuana, Laurent M.
Year: 2002   view abstract, download publication »
Publication Year: 2001
 
Title: Influence of moisture absorption on mechanical properties of wood flour- polypropylene composites
Source: Journal of thermoplastic composite materials. Vol. 14 (Sept. 2001): Pages 421-432
Author(s) Stark, Nicole
Year: 2001   view abstract, download publication »
Publication Year: 1999
 
Title: Melt-Blended Wood Fiber-Thermoplastic Composites
Source: USDA Forest Service, Forest Products Laboratory, Techlines, 1999
Author(s) Stark, Nicole
Year: 1999   view abstract, download publication »
Publication Year: 1998
 
Title: Dynamic and mechanical Properties of Agro-Fiber Based Composites
Source: Progress in woodfibre-plastic composites: emergence of a new industry.
Author(s) Caulfield, Daniel; Stark, Nicole; Feng, Daan; Sanadi, Anand
Year: 1998   view abstract, download publication »
Title: Injection molded composites from kenaf and recycled plastic
Source: [Proceedings of 1st annual American Kenaf Society Meeting, San Antonio, TX. S.l. : s.n, 1998?].:p. 38-42.
Author(s) Chow, Poo.; Bajwa, Dilpreet S.; Lu, Wen-da.; Youngquist, John A.; Stark, Nicole M.; Li, Qiang.; English, Brent.
Year: 1998   view abstract, download publication »
Title: Weight Reduction: Wood versus Mineral Fillers in Polypropylene
Source: The Fourth International Conference on Woodfiber-Plastic Composites. 1998, pp. 237-244
Author(s) English, Brent; Stark, Nicole; Clemons, Craig
Year: 1998   view abstract, download publication »
Publication Year: 1997
 
Title: Composites from Recycled Plastics and Agricultural Fibers
Source: The Fourth International Conference on Woodfiber-Plastic Composites, May 12-14, 1997 The Madison Concourse Hotel Madison, Wisconsin; pp. 294-295; 1997
Author(s) Chow, Poo; Meimban, Roger; Bajwa, Dilpreet S.; Youngquist, John A.; Stark, Nicole M.; Muehl, Jim H.; Li, Qiang; Krzysik, Andrzej M.; Engilish, Brent
Year: 1997   view abstract, download publication »
Title: Effect of Particle Size on Properties of Wood-Flour Reinforced Polypropylene Composites
Source: Fourth International conference on Woodfiver-Plastic composites, pp. 134-143
Author(s) Stark, Nicole M.; Berger, Mark J.
Year: 1997   view abstract, download publication »
Title: Effect of Species and Particle Size on Properties of Wood-Flour-Filled Polypropylene Composites
Source: Proceedings of Functional Fillers, November 1997, pp. 1-16
Author(s) Stark, Ms. Nicole; Berger, Mark J.
Year: 1997   view abstract, download publication »
Title: Heat release rate of wood-plastic composites
Source: SAMPE journal. Vol. 33, no. 5 (Sept./Oct. 1997).:p. [26]-[31].
Author(s) Stark, N. M.; White, R. H.; Clemons, C. M.
Year: 1997   view abstract, download publication »
Title: Investigations of Species Effects in an Injection-Molding-Grade, Wood-Filled Polypropylene
Source: Fourth International Conference on Woodfiber-Plastic Composites. Forest Products Society. Proceedings No. 7277. 1997. pp. 19-25
Author(s) Berger, Mark J.; Stark, Nicole M.
Year: 1997   view abstract, download publication »
Title: USDA Forest Products Laboratory Performance-Designed Composites
Source: Fourth International Conference on Woodfiber-Plastic Composites.
Author(s) Stark, Nicole M.; Clemons, Craig M.
Year: 1997   view abstract, download publication »
Publication Year: 1996
 
Title: Waste-wood-derived fillers for plastics
Source: Gen. Tech. Rep. FPL-GTR-91. Madison, WI: U.S. Department of Agriculture, Forest Service, Forest Products Laboratory. 15 p.
Author(s) English, Brent; Clemons, Craig M.; Stark, Nicole; Schneider, James P.
Year: 1996   view abstract, download publication »
Title: Wood and Mineral Fillers for Injection Molding Grade Polypropylene
Source: pp. 1-10
Author(s) English, Brent; Stark, Nicole; Clemons, Craig
Year: 1996   view abstract, download publication »
 
Publication Year: 2018
Image of composites made with modified cellulose nanofibrils (CNFs) (left) and unmodified CNFs (right). USDA Forest Service
Highlight ID: 1306
Modifying Cellulose Nanomaterials for Wet Compounding into Polylactic Acid

Cellulose nanomaterials (CNMs) have been demonstrated to significantly improve various properties, including mechanical and barrier performance, of polymer composites, but one of the major impediments for producing these cellulose nanocomposites is t ...

 
Publication Year: 2017

Highlight ID: 1271
Improving biopolymers for packaging applications using surface-tailored cellulose nanocrystals

Demand is rapidly increasing for environmentally friendly packaging materials that are derived from renewable resources and are biodegradable, but many of these "green" polymers do not perform as well as traditional, fossil fuel-derived polymers. B ...

 
Publication Year: 2016
Blown film extrusion of completely biobased poly(lactic acid) and cellulose nanocrystal polymer composites.  Sonal Karkhanis and Anna Kace Marra, Michigan State University.
Highlight ID: 654
FPL<>Renewable, Biodegradable Polylactic Acid-Cellulose Nanocrystal Composites for Packaging Applications

Packaging research conducted at the Forest Products Laboratory is aimed at developing fully biobased composites containing cellulose nanomaterials for packaging applications. Cellulose nanomaterials exhibit a number of interesting properties and have ...

 
Publication Year: 2014
This research will improve the durability of wood-plastic composite deckboards such as the one shown here being evaluated for color. Nicole Stark, USDA Forest Service
Highlight ID: 584
Wood Flour Extraction Improves Moisture Performance of Wood-Plastic Composites

Improving the moisture performance of wood-plastic composites provides a potential avenue toward improving the product's overall durability. Forest Service scientists evaluated methods for pre-treating the wood flour before incorporation into the pla ...

 
Publication Year: 2013
Beetle-killed lodgepole pine fiber treated with potassium methyl siliconate. Cheng Piao, Louisiana State University
Highlight ID: 453
Wood-Plastic Composites Improved with Fiber Pre-Treatment

Scientists determine the dimensional stability of wood-plastic composites can be improved by treating wood sawdust and particles derived from beetle-killed trees with potassium methyl siliconate before incorporating the wood into high-density polyeth ...

 
Publication Year: 2012

Highlight ID: 5
New Drying Process Gives Black Locust Wood Exotic Appearance

Heat treatment that prevents discoloration increases uses of this fast growing wood ...

 
Publication Year: 2010

Highlight ID: 170
Centennial Edition, Wood Handbook—Wood as an Engineering Material

The Wood Handbook—Wood as an Engineering Material serves as a primary reference document for a wide variety of users-from the general public through architects and design engineers who use wood in highly engineered structures. ...

Oxygen index test of a wood-plastic composite. Forest Service
Highlight ID: 161
Evaluation of Various Fire Retardants for Use in Wood Flour/Polyethylene Composites

Wood-plastic composites (WPCs) represent a class of materials increasingly used in residential construction and furniture-making. The fire performance of WPCs is not well understood, however, and there is little information regarding the effectivenes ...

TitleDate Posted
CompositesWood-Based Composite Materials

Wood-based composite materials come in many forms, including panel products, glued-laminated timbers, plywood, fiberboard, particleboard, and others...

06-18-2014