Banner for LabNotes
From Lab Notes
Contact Information
Forest Products Laboratory
One Gifford Pinchot Drive
Madison, WI 53726-2398
Phone: (608) 231-9200
Fax: (608) 231-9592
Email

 

You are here: FPL Home  / Information  / Employees Directory  / Profile

Richard Reiner
Richard Reiner

Richard Reiner

Fiber and Chemical Sciences Research
Unit: FPL-4709
Chemical Engineer
One Gifford Pinchot Drive
Madison, WI
United States
53726-2398

Phone: 608-231-9442
richard.s.reiner@usda.gov

 
Publication Year: 2015
Sequential vacuum treatment of southern pine with naturally occurring cellulose nanocrystals followed by biocide demonstrated penetration of wood before agglomeration occurred (left), but reversing the treatment sequence resulted in agglomeration on the surface of southern pine (right). USDA Forest Service
Highlight ID: 602
Cellulose Nanocrystals Chemically Entrap Biocide in Wood

Forest Service scientists evaluated naturally occurring cellulose nanocrystals (CNC) that are reported to have unique chemical properties and impart high strength were evaluated for the potential to improve durability of wood. CNC were shown to penet ...