Banner for LabNotes
From Lab Notes
Contact Information
Forest Products Laboratory
One Gifford Pinchot Drive
Madison, WI 53726-2398
Phone: (608) 231-9200
Fax: (608) 231-9592
Email

 

You are here: FPL Home  / Information  / Employees Directory  / Profile

Rebecca E. Ibach
Rebecca E. Ibach

Rebecca E. Ibach

Forest Biopolymer Science and Engineering
Unit: FPL-4707
Research Chemist
One Gifford Pinchot Drive
Madison, WI
United States
53726-2398

Phone: 608-231-9472
Fax: 608-231-9262
rebecca.e.ibach@usda.gov

Research Interest

  • Chemical modification for improvement of wood properties
  • Solid wood polymer composites
  • Integrated approach to wood protection
  • Woodfiber-plastic composites durability:
  • laboratory and field evaluations


Education

  • University of Wisconsin Madison, Ph.D. Wood Chemistry ,

Below are the 81 US Forest Service publications sorted by year. You may re-sort the list by: Title, Date Posted, Category, Publication or Year.

Publication Year: 2022
 
Title: Small Angle Neutron Scattering Reveals Wood Nanostructural Features in Decay Resistant Chemically Modified Wood
Source: Frontiers in Forests and Global Change journal
Author(s) Ibach, Rebecca E.; Plaza, Nayomi Z.; Pingali, Sai Venkatesh.
Year: 2022   view abstract, download publication »
Publication Year: 2021
 
Title: Characterization of the supramolecular structures of cellulose nanocrystals of different origins
Source: Cellulose
Author(s) Agarwal, Umesh P.; Reiner, Richard S.; Ralph, Sally A.; Catchmark, Jeffery ; Chi, Kai ; Foster, E. Johan; Hunt, Christopher G.; Baez, Carlos ; Ibach, Rebecca E.; Hirth, Kolby C.
Year: 2021   view abstract, download publication »
Title: Comparative Adhesive Bonding of Wood Chemically Modified with either Acetic Anhydride or Butylene Oxide
Source: Forests
Author(s) Frihart, Charles R.; Brandon, Rishawn ; Ibach, Rebecca E.; Hunt, Christopher G.; Gindl-Altmutter, Wolfgang
Year: 2021   view abstract, download publication »
Title: Probing the nanostructural mechanisms behind decay resistance of chemically modified wood using small angle neutron scattering
Source: Proceedings paper
Author(s) Plaza Rodriguez, Nayomi; Ibach, Rebecca; Pingali, Sai Venkatesh
Year: 2021   view abstract, download publication »
Title: Specialty treatments
Source: Chapter 19 in FPL-GTR-282
Author(s) Ibach, Rebecca
Year: 2021   view abstract, download publication »
Title: USDA Forest Service Forest Products Laboratory: Acetylation of Wood 1945–1966
Source: Forests
Author(s) Ibach, Rebecca E.; Rowell, Roger M.
Year: 2021   view abstract, download publication »
Title: Using Thermal Neutron Imaging in Forest Products Research
Source: Environmental Sciences Proceedings
Author(s) Plaza, Nayomi Z.; Ibach, Rebecca E.; Hasburgh, Laura E.; Taylor, Michael
Year: 2021   view abstract, download publication »
Publication Year: 2020
 
Title: Long-term field exposure of wood-plastic composites processed on a commercial-size extruder
Source: Ibach, Rebecca E.; Clemons, Craig M.; Stark, Nicole M. 2020. Long-term field exposure of wood-plastic composites processed on a commercial-size extruder. Proceedings, 51st annual meeting of the international research group on wood protection . June, 10-11, 2020. 11 p.
Author(s) Ibach, Rebecca E.; Clemons, Craig M.; Stark, Nicole M.
Year: 2020   view abstract, download publication »
Publication Year: 2019
 
Title: The life and work of Bruce Johnson at the Forest Products Laboratory and in the American Wood Protection Association
Source: In: Proceedings, 115th annual meeting of the American Wood Protection Association. Birmingham, AL: American Wood Protection Association: 100-104.
Author(s) Kirker, Grant ; Ibach, Rebecca E.
Year: 2019   view abstract, download publication »
Title: Using x-ray scattering to elucidate the mechanisms behind the moisture and fungal decay resistance of epoxybutene modified wood
Source: In: Proceedings, 2019 IRG annual meeting. Stockholm, Sweden: The International Research Group on Wood Protection. 15 p.
Author(s) Ibach, Rebecca E.; Plaza, Nayomi
Year: 2019   view abstract, download publication »
Publication Year: 2018
 
Title: Effects of Teak, Tectona grandis Linn, heartwood extractives against Heterotermes indicola (Isoptera: Rhinotermitidae)
Source: Proceedings, IRG annual meeting. The International Research Group on Wood Protection. 1-16.
Author(s) Hassan, Babar ; Ahmed, Sohail ; Mankowski, Mark , E. .; Kirker, Grant ; Ibach, Rebecca ; Misbah ul Haq, Muhammad
Year: 2018   view abstract, download publication »
Title: Production of high lignin-containing and lignin-free cellulose nanocrystals from wood
Source: Cellulose. 25(10): 5791-5805.
Author(s) Agarwal, Umesh P.; Ralph, Sally A.; Reiner, Richard S.; Hunt, Christopher G.; Baez, Carlos ; Ibach, Rebecca ; Hirth, Kolby C.
Year: 2018   view abstract, download publication »
Title: Stable and durable wood products based on molecular modification
Source: Journal of Tropical Forest Science. 30(5): 488-495.
Author(s) Rowell, RM ; Ibach, RE
Year: 2018   view abstract, download publication »
Title: Termite resistance of wood-plastic composites made with acetylated wood flour, coupling agent or zinc borate
Source: In: Proceedings, IRG annual meeting. The International Research Group on Wood Protection. 11 p.
Author(s) Ibach, Rebecca E.; Hadi, Yusuf Sudo; Clemons, Craig M.; Sulaeman, Yusuf
Year: 2018   view abstract, download publication »
Publication Year: 2017
 
Title: Adhesives for Achieving Durable Bonds with Acetylated Wood
Source: Polymers. 9(12): 731-743.
Author(s) Frihart, Charles; Brandon, Rishawn; Beecher, James; Ibach, Rebecca
Year: 2017   view abstract, download publication »
Title: Laboratory and environmental decay of wood–plastic composite boards: flexural properties
Source: Wood Material Science & Engineering. 54(4): 1-16.
Author(s) Ibach, Rebecca; Gnatowski, Marek; Sun, Grace; Glaeser, Jessie; Leung, Mathew; Haight, John
Year: 2017   view abstract, download publication »
Title: Long term durability of wood-plastic composites made with chemically modified wood
Source: In: Advancements in fiber-polymer composites conference proceedings. Madison, WI: 1-17.
Author(s) Ibach, Rebecca E.; Clemons, Craig M.
Year: 2017   view abstract, download publication »
Title: The use of new, aqueous chemical wood modifications to improve the durability of wood-plastic composites
Source: Forty-eighth Annual Meeting of the International Research Group on Wood Protection. 2017 June 4-8; Ghet, Belgium. pp. 1-9
Author(s) Ibach, Rebecca E.; Clemons, Craig M.; Chen, George C.
Year: 2017   view abstract, download publication »
Publication Year: 2016
 
Title: Exterior Decay of Wood-Plastic Composite Boards: Characterization and Magnetic Resonance Imaging
Source: Forest Products Journal
Author(s) Ibach, Rebecca; Sun, Grace; Gnatowski, Marek; Glaeser, Jessie; Leung, Mathew; Haight, John
Year: 2016   view abstract, download publication »
Title: Laboratory and exterior decay of wood plastic composite boards: voids analysis and computed tomography
Source: Wood Material Science & Engineering
Author(s) Sun, Grace; Ibach, Rebecca E.; Faillace, Meghan; Gnatowski, Marek; Glaeser, Jessie A.; Haight, John
Year: 2016   view abstract, download publication »
Publication Year: 2015
 
Title: Wood properties influence bond durability
Source: Proceedings of the 5th International Scientific Conference on Hardwood Processing 2015, Sept. 15-17, 2015 pp. 78-84; 2015
Author(s) Frihart, Charles R.; Yelle, Daniel J.; Ibach, Rebecca E.
Year: 2015   view abstract, download publication »
Publication Year: 2014
 
Title: Chemical Modification of Kraft Lignin: Effect on Chemical and Thermal Properties
Source: BioResources, Volume 9, Number 3, 2047; pp. 5488-5500.
Author(s) Chen, Yao; Stark, Nicole M.; Cai, Zhiyong; Frihart, Charles R.; Lorenz, Linda F.; Ibach, Rebecca E.
Year: 2014   view abstract, download publication »
Title: Decay resistance of wood-plastic composites reinforced with extracted or delignified wood flour
Source: IRG/WP 14-40655, THE INTERNATIONAL RESEARCH GROUP ON WOOD PROTECTION Section 4, Processes and properties, Paper prepared for the 45th IRG Annual Meeting St George, Utah, USA, 11-15 May, 2014 pp. 2-9.
Author(s) Ibach, Rebecca E.; Chen, Yao; Stark, Nicole M.; Tshabalala, Mandla A.; Fan, Yongming; Gao, Jianmin
Year: 2014   view abstract, download publication »
Title: Degradation Behavior and Accelerated Weathering of Composite Boards Produced from Waste Tetra Pak® Packaging Materials
Source: BioResources, Volume 9, Number 3, 2014; pp. 4784-4807.
Author(s) Yilgor, Nural; Kose, Coskun; Terzi, Evren; Figen, Aysel Kanturk; Ibach, Rebecca; Kartal, S. Nami; Piskin, Sabriye
Year: 2014   view abstract, download publication »
Title: Magnetic resonance imaging used for the evaluation of water presence in wood plastic composite boards exposed to exterior conditions
Source: Wood Material Science and Engineering, 2014; 18p.
Author(s) Gnatowski, Marek; Ibach, Rebecca; Leung, Mathew; Sun, Grace
Year: 2014   view abstract, download publication »
Title: Modern Instrumental Methods to Investigate the Mechanism of Biological Decay in Wood Plastic Composites
Source: IRG/WP 14-40674, The international Research Group on Wood Protection, section 4, Processes and properties, Paper prepared for the 45th IRG Annual Meeting, St George, Utah, USA, 11-15 May 2014; pp. 2-20;.
Author(s) Sun, Grace; Ibach, Rebecca; Gnatowski, Marek; Glaeser, Jessie; Leung, Mathew; Haight, John
Year: 2014   view abstract, download publication »
Title: Strength loss in decayed wood
Source: In: the McGraw-Hill Encyclopedia of Science & Technology, 2014; pp. 368-371.
Author(s) Ibach, Rebecca E.; Lebow, Patricia K.
Year: 2014   view abstract, download publication »
Title: Thermal behavior of extracted and delignified pine wood flour
Source: Thermochimica Acta Volume 591, 2014; pp. 40–44.
Author(s) Chen, Yao; Tshabalala, Mandla A.; Gao, Jianmin; Stark, Nicole M.; Fan, Yongming; Ibach, Rebecca E.
Year: 2014   view abstract, download publication »
Publication Year: 2013
 
Title: Chapter 5:Biological Properties of Wood
Source: In: Handbook of Wood Chemistry and Wood Composites, second edition, CRC press. 2013. pp. 99-126.
Author(s) Ibach, Rebecca E.
Year: 2013   view abstract, download publication »
Title: Chemically imaging the effects of the addition of nanofibrillated cellulose on the distribution of poly(acrylic acid) in poly(vinyl alcohol)
Source: Polymer, 2013. pp.1-4.
Author(s) Clemons, Craig; Sedlmair, Julia; Illman, Barbara; Ibach, Rebecca; Hirschmugl, Carol
Year: 2013   view abstract, download publication »
Title: Effect of environmental conditions on the mechanical properties and fungal degradation of polycaprolactone/microcrystalline cellulose/wood flour composites
Source: BioResources Volume 8, Number 3, pp.3322-3335; 2013
Author(s) Sabo, Ronald; Jin, Liwei; Stark, Nicole; Ibach, Rebecca E.
Year: 2013   view abstract, download publication »
Title: Field and Laboratory Decay Evaluations of wood-plastic Composites
Source: Forest Prod. J. Volume 63, Number 3/4, pp. 76–87.
Author(s) Ibach, Rebecca E.; Gnatowski, Marek; Sun, Grace
Year: 2013   view abstract, download publication »
Title: Moisture and Fungal Durability of Wood-Plastic Composites Made With Chemically Modified and Treated Wood Flour
Source: THE INTERNATIONAL RESEARCH GROUP ON WOOD PROTECTION, Section 4, Processes and Properties, IRG/WP 13-40648; 2013; 8 p.
Author(s) Segerholm, B. Kristoffer; Ibach, Rebecca E.
Year: 2013   view abstract, download publication »
Title: Thermal Properties of Extracted and Delignified Wood Flour for use in Wood-Plastic Composites
Source: In: Conference Proceedings, The Advancements in Fiber-Polymer Composites: Wood Fiber, Natural Fibers and Nanocellulose, May 6-7, 2013 Milwaukee, Wisconsin. 10 p.
Author(s) Chen, Yao; Tshabalala, Mandla A.; Stark, Nicole M.; Gao, Jianmin; Fan, Yongming; Ibach, Rebecca E.
Year: 2013   view abstract, download publication »
Publication Year: 2012
 
Title: Chapter 16 Lumen Modification
Source: In: Second edition of the Handbood of wood Chemistry and Wood Composites, Chapter 16, Roger Rowell, Editor, by CRC Books, 2013. pp. 599-625.
Author(s) Ibach, Rebecca E.; Rowell, Roger M.
Year: 2012   view abstract, download publication »
Title: Moisture Sorption in Artificially aged wood-plastic composites
Source: BioResources Volume 7, Number 1, 1283-1293; 2012.
Author(s) Segerholm, B. Kristoffer; Ibach, Rebecca E.; Wålinder, Magnus E.P.
Year: 2012   view abstract, download publication »
Title: Moisture Sorption, Biological Durability, and Mechanical Performance of WPC Containing Modified Wood and Polylactates
Source: BioResources Volume 7, Number 4, 4575-4585; 2012.
Author(s) Segerholm, B. Kristoffer; Ibach, Rebecca E.; Westin, Mats
Year: 2012   view abstract, download publication »
Title: Wood preservative testing
Source: McGraw-Hill Yearbook of Science & Technology; pp.317-319; 2012
Author(s) Ibach, Rebecca; Lebow, Stan T.
Year: 2012   view abstract, download publication »
Publication Year: 2011
 
Title: Durability of PLA-modified wood composites
Source: Proceedings of the 11th international conference on wood and biofiber plastic composites & nanotechnology in wood composites symposium, 2011 May 16-17, Madison, WI. Madison, WI : Forest Products Society, 2011: [3] p. [1 flash drive]
Author(s) Kristoffer, Segerholm B.; Ibach, Rebecca E.; Westin, Mats
Year: 2011   view abstract, download publication »
Title: The Use of Esterified Lignin for Synthesis of Durable Composites
Source: In: Proceedings of the 7th meeting of the NORDIC-BALTIC NETWORK IN WOOD MATERIAL SCIENCE & ENGINEERING (WSE) October 27-28, 2011, Oslo, Norway, 2011, pp. 173-178; 2011.
Author(s) Olsson, S.; Ostmark, E.; Ibach, R.E.; Clemons, C.M.; Segerholm, K.B.; Englund, F.
Year: 2011   view abstract, download publication »
Publication Year: 2010
 
Title: .Wood Handbook, Wood as an Engineering Material (All Chapters)
Source: Forest Products Laboratory. Wood handbook - Wood as an engineering material. General Technical Report FPL-GTR-190. Madison, WI: U.S. Department of Agriculture, Forest Service, Forest Products Laboratory: 508 p. 2010
Author(s) Bergman, Richard; Cai, Zhiyong; Carll, Charlie G.; Clausen, Carol A.; Dietenberger, Mark A.; Falk, Robert H.; Frihart, Charles R.; Glass, Samuel V.; Hunt, Christopher G.; Ibach, Rebecca E.; Kretschmann, David E.; Rammer, Douglas R.; Ross, Robert J.; Star
Year: 2010   view abstract, download publication »
Title: Chapter 8 Wood Durability and Stability Without Toxicity
Source: In: Sustainable Development in the Forest Products Industry; Roger M. Rowell :: Fernando Caldeira :: Judith K. Rowell; 2010
Author(s) Rowell, Roger M.; Ibach, Rebecca E.; Nilsson, Thomas
Year: 2010   view abstract, download publication »
Title: Durability of wood-plastic composite lumber
Source: In: McGraw-Hill Yearbook of Science & Technology 2010; pp. 113-116; 2010
Author(s) Ibach, Rebecca E.
Year: 2010   view abstract, download publication »
Title: Laboratory Evaluation of Borate/Amine/Zinc Formulations in Wood for Fungal Decay Protection
Source: In: Proceedings of the 106 annual meeting of the American Wood Protection Association, Hyatt Regency Riverfront, Savannah, Georgia May 23-25, 2010, Volume 106, pp. 139-145; 2010
Author(s) Chen, George C.; Ibach, Rebecca E.
Year: 2010   view abstract, download publication »
Title: Performance Enhancement of Wood Surfaces Used in Outdoor Applications: The Effect of Sol-gel Treatment on the Weathering Performance of Solid Wood-polymer Composites
Source: The Fifth European Conference on Wood Modification, September 20-21, 2010. pp. 355-362
Author(s) Ibach, Rebecca E.; Tshabalala, Mandla A.; Starr, Charles
Year: 2010   view abstract, download publication »
Title: Synthesis and Evaluation of Dioctylaminoborate in Wood for Brown Rot Decay Protection
Source: In: Proceedings of the 106 annual meeting of the American Wood Protection Association, Hyatt Regency Riverfront, Savannah, Georgia May 23-25, 2010, Volume 106, pp. 134-138; 2010
Author(s) Chen, George C.; Ibach, Rebecca E.
Year: 2010   view abstract, download publication »
Title: Wood Handbook, Chapter 19: Specialty Treatments
Source: General Technical Report FPL-GTR-190. Madison, WI: U.S. Department of Agriculture, Forest Service, Forest Products Laboratory: 19-1 - 19-16. Chapter 19.
Author(s) Ibach, Rebecca E.
Year: 2010   view abstract, download publication »
Publication Year: 2009
 
Title: Evaluating Physical Property Changes for Small-Diameter, Plantation-Grown Southern Pine after In Situ Polymerization of an Acrylic Monomer
Source: Forest Prod. J. 59(10):64-71.
Author(s) Bergman, Richard; Ibach, Rebecca E.; LaPasha, Constatine; Denig, Joseph
Year: 2009   view abstract, download publication »
Title: Understanding Decay Resistance, Dimensional Stability and Strength Changes in Heat Treated and Acetylated Wood
Source: Rowell, R.M., Ibach, R.E., McSweeny, J., and Nilsson, T. 2009. Understanding decay resistance, dimensional stability and strength changes in heat treated and acetylated wood. 2009 European Conference on Wood Modification, April 27-29, 2009, Stockholm, Sweden. Pp. 489-502 (refereed); 2009
Author(s) Rowell, Roger M.; Ibach, Rebecca E.; McSweeny, James; Nilsson, Thomas
Year: 2009   view abstract, download publication »
Title: Understanding decay resistance, dimensional stability and strength changes in heat-treated and acetylated wood
Source: Wood Material Science and Engineering, 2009; 1-2: 14-22
Author(s) Rowell, Roger M.; Ibach, Rebecca E.; McSweeny, James; Nilsson, Thomas
Year: 2009   view abstract, download publication »
Publication Year: 2008
 
Title: Biological degradation of wood-plastic composites (WPC) and strategies for improving the resistance of WPC against biological decay
Source: Development of commercial wood preservatives : efficacy, environmental, and health issues. Washington, DC : American Chemical Society ; [New York] : Distributed by Oxford University Press, c2008. ACS symposium series ; 982: ISBN: 0841239517: 9780841239
Author(s) Schirp, Anke; Ibach, Rebecca E.; Pendleton, David E.; Wolcott, Michael P.
Year: 2008   view abstract, download publication »
Publication Year: 2007
 
Title: Influence of Moisture on Brown-Rot Fungal Attack on Wood
Source: Proceedings of the 3rd meeting of the NORDIC-BALTIC NETWORK IN WOOD MATERIAL SCIENCE AND ENGINEERING (WSE) October 29-30,2007, Helsinki, Finland.ISBN 951-45-9098-8 pp.65-69; 2007
Author(s) Rowell, Ibach, Nilsson
Year: 2007   view abstract, download publication »
Title: What does bonding to modified wood tell us about adhesion?
Source: IN: Bonding of modified wood: proceedings of the 5th COST E34 International Workshop, Bled, Slovenia, Sept. 6th, 2007. Ljubljana : Biotechnical Faculty, Dept. of Wood Science and Technology, 2007. ISBN13: 9789616144179. ISBN: 9616144170. 10 p.
Author(s) Hunt, Christopher G. , Rishawn Brandon, Rebecca E. Ibach, Charles R. Frihart
Year: 2007   view abstract, download publication »
Title: Wood-plastic composites with reduced moisture : effects of chemical modification on durability in the laboratory and field
Source: Ninth International Conference on Wood & Biofiber Plastic Composites : May 21-23, 2007 ... Madison, Wisconsin, USA. Madison, WI : Forest Products Society, c2007: ISBN: 1892529505: 9781892529503: Pages 259-266
Author(s) Ibach, Rebecca E.; Clemons, Craig M.; Schumann, Rebecca L.
Year: 2007   view abstract, download publication »
Publication Year: 2006
 
Title: Effect of acetylated wood flour or coupling agent on moisture, UV, and biological resistance of extruded woodfiber-plastic composites
Source: Wood protection 2006 : March 21-23, 2006 ... New Orleans, Louisiana, USA. Madison, WI : Forest Products Society, 2006: Pages 139-147
Author(s) Ibach, Rebecca E.; Clemons, Craig M.
Year: 2006   view abstract, download publication »
Publication Year: 2005
 
Title: Biological properties
Source: Handbook of wood chemistry and wood composites. Boca Raton, Fla. : CRC Press, 2005: pages 99-120.
Author(s) Ibach, Rebecca E.
Year: 2005   view abstract, download publication »
Title: Effects of chemically modified wood on bond durability
Source: Wood Adhesives 2005 : November 2-4, 2005 ... San Diego, California, USA. Madison, WI : Forest Products Society, 2005: ISBN: 1892529459: pages 111-114.
Author(s) Brandon, Rishawn; Ibach, Rebecca E.; Frihart, Charles R.
Year: 2005   view abstract, download publication »
Title: Lumen modifications
Source: Handbook of wood chemistry and wood composites. Boca Raton, Fla. : CRC Press, 2005: pages 421-446.
Author(s) Ibach, Rebecca E.; Ellis, W. Dale
Year: 2005   view abstract, download publication »
Publication Year: 2004
 
Title: Effects of processing method and moisture history on laboratory fungal resistance of wood-HDPE composites
Source: Forest Prod. J. 54(4):50-57.
Author(s) Clemons, Ibach
Year: 2004   view abstract, download publication »
Title: Effects of processing method and moisture history on laboratory fungal resistance of wood-HDPE composites.
Source: Forest products journal. Vol. 54, no. 4 (Apr. 2004): Pages 50-57.
Author(s) Clemons, Craig M.; Ibach, Rebecca E.
Year: 2004   view abstract, download publication »
Title: Rapid analysis of the chemical composition of agricultural fibers using near infrared spectroscopy and pyrolysis molecular beam mass spectrometry
Source: Biomass and bioenergy. Vol. 27 (2004): Pages 77-88
Author(s) Kelley, Stephen S.; Rowell, Roger M.; Davis, Mark; Jurich, Cheryl K.; Ibach, Rebecca
Year: 2004   view abstract, download publication »
Title: SELECTIVITY OF BONDING FOR MODIFIED WOOD
Source: In: Proceedings of the 27th annual meeting of the Adhesion Society. 2004. pp. 329-331
Author(s) Frihart; Brandon; Ibach
Year: 2004   view abstract, download publication »
Publication Year: 2003
 
Title: Application of laboratory fungal resistance tests to solid wood and wood-plastic composite
Source: Plastics in building construction. Vol. 27, no. 2 (Feb. 2003): pages 7-14
Author(s) Clemons, Craig Merrill; Ibach, Rebecca E.
Year: 2003   view abstract, download publication »
Title: Combined ultraviolet and water exposure as a preconditioning method in laboratory fungal durability testing
Source: Seventh International Conference on Woodfiber-Plastic Composites (and other natural fibers), May 19-20, 2003 ... Madison, Wisconsin, USA. Madison, WI : Forest Products Society, 2003: Pages 61-67
Author(s) Ibach, Rebecca E.; Clemons, Craig M.; Stark, Nicole M.
Year: 2003   view abstract, download publication »
Title: Wood preservation
Source: McGraw-Hill yearbook of science & technology 2003. New York : McGraw-Hill, c2003: pages 469-471.
Author(s) Ibach, Rebecca E.
Year: 2003   view abstract, download publication »
Publication Year: 2002
 
Title: Biological resistance of polyethylene composites made with chemically modified fiber or flour
Source: Proceedings of the 6th Pacific Rim Bio-Based Composites Symposium & Workshop on the Chemical Modification of Cellulosics, Portland, Oregon, USA, 2002: pages 574-584.
Author(s) Ibach, Rebecca E.; Clemons, Craig M.
Year: 2002   view abstract, download publication »
Title: Effect of Wet-Dry Cycling on the Decay Properties of Aspen Fiber High-Density Polypropylene Composites
Source: In: Sixth International Conference on Woodfiber-Plastic Composites May 15-16,2001 The Madison Concourse Hotel Madison, Wisconsin; pp. 267-270
Author(s) Ibach, Rowell, Lange, Schumann
Year: 2002   view abstract, download publication »
Title: Laboratory tests on fungal resistance of wood filled polyethylene composites
Source: ANTEC 2002 Annual Tecnical Conference : May 5-9, 2002, San Francisco, CA. : conference proceedings. Volume II, Materials. S.l. : Society of Plastics Engineers, 2002: p. 2219-2222
Author(s) Clemons, Craig M.; Ibach, Rebecca E.
Year: 2002   view abstract, download publication »
Title: The effect on biological and moisture resistance of epichlorohydrin chemically modified wood
Source: Thirty-third annual meeting of the International Research Group on Wood Preservation, 2002 May 12-17, Cardiff, South Wales, UK. Stockholm, Sweden : IRG Secretariat, [2002]: 11 pages.
Author(s) Ibach, Rebecca E.; Lee, Beom-Goo
Year: 2002   view abstract, download publication »
Publication Year: 2001
 
Title: Wood preservation based on in situ polymerization of bioactive monomers: Part 1. Synthesis of bioactive monomers, wood treatments and microscopic analysis
Source: Journal
Author(s) Ibach, Rebecca
Year: 2001   view abstract, download publication »
Title: Wood preservation based on in situ polymerization of bioactive monomers: Part 2. fungal resistance and thermal properties of treated wood.
Source: Journal
Author(s) Ibach, Rebecca
Year: 2001   view abstract, download publication »
Publication Year: 2000
 
Title: Decay protection based on moisture exclusion resulting from chemical modification of wood
Source: Conference proceedings
Author(s) Ibach, Rebecca
Year: 2000   view abstract, download publication »
Title: Improvements in decay resistance based on moisture exclusion
Source: Mol. Cryst. And Liq. Crsyt., 2000. 353: 23-33.
Author(s) Rowell, Roger M.; Ibach, Rebecca E.
Year: 2000   view abstract, download publication »
Title: Termite and fungal resistance of in situ polymerized tributyltin acrylate and acetylated Indonesian and USA wood
Source: [The International Research Group on Wood Preservation. Section 3, Wood Protecting Chemicals : 31st annual meeting, Kona, Hawaii, USA, 14-19 May 2000. Stockholm, Sweden : IRG Secretariat, 2000].:13 p. : ill.
Author(s) Ibach, Rebecca E.; Hadi, Yusuf Sudo.; Nandika, Dodi.; Yusuf, Sulaeman.; Indrayani, Yuliati.
Year: 2000   view abstract, download publication »
Publication Year: 1995
 
Title: Low polymer levels containing bioactive monomer polymerized in situ provide resistance to Gloeophyllum trabeum
Source: Document No. IRG/WP/95-30066. International Research Group on Wood Preservation Twenty-Sixth Annual Meeting, Helsingor, Denmark. 17 p.
Author(s) Ibach, Rebecca E.; Rowell, Roger M.
Year: 1995   view abstract, download publication »
Publication Year: 1992
 
Title: Effect of salt water evaporation on tracheid separation from wood surfaces
Source: Forest Products Journal, Vol. 42, No. 7/8: 1992 ; pp.57-59
Author(s) Johnson, Bruce R.; Ibach, Rebecca E.; Baker, Andrew J.
Year: 1992   view abstract, download publication »
Publication Year: 1991
 
Title: Characteristics of Cotton Cellulose Depolymerized by a Brown-Rot Fungus, by Acid, or by Chemical Oxidants
Source: Holzforschung, Vol. 45, 1991, No. 4, pp. 239-244
Author(s) Kirk, T. Kent; Ibach, Rebecca; Mozuch, Michael D.; Conner, Anthony H.; Highley, Terry L.
Year: 1991   view abstract, download publication »
Publication Year: 1990
 
Title: Characterization of palo podrido, a natural process of delignification in wood
Source: Applied and Environmental Microbiology. 56(91): 65-74.
Author(s) Agosan, Eduardo ; Blanchette, Robert A.; Silva, Herman ; Lapierre, Catherine ; Cease, Kory R.; Ibach, Rebecca E.; Abad, André R.; Muga, Pedro
Year: 1990   view abstract, download publication »
Publication Year: 1989
 
Title: Effect of Brown-Rot Fungi on Cellulose
Source: BIODETERIORATION RESEARCH
Author(s) Highley, T.L.; Kirk, T.K.; Ibach, R.
Year: 1989   view abstract, download publication »
Title: Identification of terminal structures in cellulose degraded by the brown-rot fungus Postia placenta
Source: Document No. IRG/WP/1389. International Research Group on Wood Preservation Twentieth Annual Meeting, Lappeenranta, Finland, May 21-26, 1989. 5 p.
Author(s) Kirk, T.K. ; Highley, T.L. ; Ibach, R. ; Mozuch, M.D.
Year: 1989   view abstract, download publication »
Publication Year: 1988
 
Title: Properties of Cellulose Degraded by the Brown-Rot Fungus, Postia plancenta
Source: The International Research Group on Wood Preservation, Document No.: IRG/WP/1350. 1988.
Author(s) Highley, Terry L.; Ibach, Rebecca; Kirk, T.Kent
Year: 1988   view abstract, download publication »
 
Publication Year: 2018
Laboratory subterranean termite test (Coptotermes curvignathus Holmgren) with five wood-plastic composites blends and untreated pine wood. Bogor Agricultural University, Indonesia
Highlight ID: 1304
Termite Resistance of WoodPlastic Composites

Wood-plastic composite (WPC) specimens were exposed to termites both in the laboratory and the field in Bogor, Indonesia. On a scale of 0 (complete failure) to 10 (sound), after 30 months field exposure, the WPC made with acetylated wood flour had no ...

 
Publication Year: 2011
Surface color of modified (B, C, D) and unmodified (A) western red cedar before (0 h) and after (720 h) of artificial weathering in a WeatherOmeter. Steve Schmieding, Forest Service
Highlight ID: 305
Lumen filling and sol-gel reinforcement of the wood cell wall

FPL researchers used a two-prong strategy to enhance weathering properties of wood. This dual treatment showed promise in protecting wood against the combined effects of sunlight and moisture. ...

 
Publication Year: 2010

Highlight ID: 170
Centennial Edition, Wood Handbook—Wood as an Engineering Material

The Wood Handbook—Wood as an Engineering Material serves as a primary reference document for a wide variety of users-from the general public through architects and design engineers who use wood in highly engineered structures. ...

TitleDate Posted
Rebecca Ibach, FPL research chemistBiological Properties of Wood

Rebecca Ibach, research chemist at FPL, has written a chapter for the new edition of the Handbook of Wood Chemistry and Wood Composites (2nd ed., 2013) titled Biological Properties of Wood...

08-13-2013