Researchers at the Forest Products Laboratory (FPL) have partnered with the World Wildlife Fund (WWF) to investigate whether wood from products sold in the United States is accurately labeled. The forensic expertise of FPL botanist Alex Wiedenhoeft was key in this research, and the findings of the study were recently published in a journal article in PLOS One.
For an easily-accessible explanation of the research, check out this story from WWF. It’s full of great photos that give you a behind-the-scenes look into Alex’s forensic work and the world’s largest research wood collection, housed here at FPL in the Center for Wood Anatomy Research.