A Salty Tale of Wood Damage Research and Discovery

A tenacious fungus, a conspiracy theory, a historic ship, a unique gift from Princeton University, and two Forest Products Laboratory (FPL) researchers, Grant Kirker and Samuel Zelinka, collaborating with researchers from Germany and Canada all converged in the right order of events to produce some of the most significant advances in wood salt damage understanding in over twenty years.

Samuel Zelinka – Supervisory Materials Research Engineer
Grant Kirker – Research Forest Products Technologist

A recent publication, “Salt Damage in Wood: Controlled Laboratory Exposures and Mechanical Property Measurements,” is the result of all of these circumstances and characters clashing and aligning.

Continue reading