Forest Products Laboratory (FPL) researcher Junyong (J.Y.) Zhu was featured in the journal Nature for his contribution to the recent article, “Developing fibrillated cellulose as a sustainable technological material.”
Fibrillated cellulose has the unique characteristics and sustainable properties that could make it the building block polymer of the very near future.
A polymer is a material used in the manufacture of innumerable commercial products, from grocery bags to automobile parts to construction materials to the brush that runs through your hair every morning. Basically, a polymer is a fabrication building block. Currently, commercial polymers are sourced primarily from metal and petroleum.