The article “Lightweight Strong Moldable Wood Via Cell Wall Engineering as a Sustainable Structural Material,” coauthored by Forest Products Laboratory research scientists Junyong Zhu, Vina Yang, and Marco Lo Ricco, with lead author Prof. Liangbing Hu at the University of Maryland-College Park, was published in the Oct. 22, 2021 issue of Science Magazine as the cover article.
“In this work,” the article states, “we demonstrate how cell wall engineering can render wood foldable and moldable while simultaneously improving its mechanical properties – endowing wood with a structural versatility previously limited to plastics and metals.”