Big Grant Funding Awarded to Tiniest, Mightiest Building Material of the Future

The Forest Products Laboratory is pleased to announce the littlest big news that could help change how we fabricate the world around us.

CN-enhanced concrete looks and acts like traditional concrete but is much stronger. Photo by Michael Goergen, U.S. Endowment.

USDA Forest Service Forest Products Laboratory (FPL) in collaboration with P3Nano from the US Endowment for Forests and Communities(U.S. Endowment) announced ten awards this month for projects ranging from one to five years, totaling $2.4 million in grants to further nanocellulose research.

The partnership funds research to evaluate the safety of cellulosic nanomaterials (CNs), develop process improvements to reduce production cost, and provide new market opportunities for advanced applications. Everything from biodegradable snack packaging to concrete additives that significantly reduce CO2 emissions are possible with CN innovation.

Continue reading