Renewable Energy Flooring Takes a Step Forward at Union South

The University of Wisconsin released the following article by Will Cushman about the advancement of a project the Forest Products Laboratory has been a collaborator on. Read on to see how simply walking on a wood floor can generate electricity!

Visitors to UW–Madison’s Union South walk across a section of floor designed and installed by College of Engineering researchers to capture the energy of footsteps and turn it into usable electricity. Photo: Adrienne Nienow

As thousands of visitors each day walk across a new flooring installation in UW–Madison’s Union South this fall, they might not realize they’re participating in what could very well represent a leap into the future of renewable energy production.

A research team led by Xudong Wang, a University of Wisconsin–Madison professor of materials science and engineering, in collaboration with the UW–Madison Grainger Institute for Engineering, has installed a high-tech flooring prototype that harvests the energy of footsteps and converts it into electricity. Continue reading

‘Shocking’ Discovery: Nanocellulose Can Turn Footsteps into Electricity

Many exciting developments have resulted from the Forest Products Laboratory (FPL) and the University of Wisconsin (UW) working together to find applications for nanocellulose. From computer chips made of wood to aerogels that could clean up oil spills, the technologies researchers dream up are fascinating.

This week, yet another discovery from this FPL/UW collaboration was unveiled: flooring that converts footsteps to usable energy.

The following is a press release from the UW on this newest development in the world of nanocellulose.

————————————————————-

Move over, solar: The next big renewable energy source could be at our feet

Flooring can be made from any number of sustainable materials, making it, generally, an eco-friendly feature in homes and businesses alike.

Now, flooring could be even more “green,” thanks to an inexpensive, simple method developed by University of Wisconsin-Madison materials engineers that allows them to convert footsteps into usable electricity.

Associate Professor Xudong Wang holds a prototype of the researchers’ energy harvesting technology, which uses wood pulp and harnesses nanofibers. The technology could be incorporated into flooring and convert footsteps on the flooring into usable electricity. Credit: Stephanie Precourt/UW-Madison

Associate Professor Xudong Wang holds a prototype of the researchers’ energy harvesting technology, which uses wood pulp and harnesses nanofibers. The technology could be incorporated into flooring and convert footsteps on the flooring into usable electricity. Credit: Stephanie Precourt/UW-Madison

Xudong Wang, an associate professor of materials science and engineering at UW-Madison, his graduate student Chunhua Yao, and their collaborators published details of the advance Sept. 24 in the journal Nano Energy.

The method puts to good use a common waste material: wood pulp. The pulp, which is already a common component of flooring, is partly made of cellulose nanofibers. They’re tiny fibers that, when chemically treated, produce an electrical charge when they come into contact with untreated nanofibers.

When the nanofibers are embedded within flooring, they’re able to produce electricity that can be harnessed to power lights or charge batteries. And because wood pulp is a cheap, abundant and renewable waste product of several industries, flooring that incorporates the new technology could be as affordable as conventional materials.

While there are existing similar materials for harnessing footstep energy, they’re costly, nonrecyclable, and impractical at a large scale.

Wang’s research centers around using vibration to generate electricity. For years, he has been testing different materials in an effort to maximize the merits of a technology called a triboelectric nanogenerator (TENG). Triboelectricity is the same phenomenon that produces static electricity on clothing. Chemically treated cellulose nanofibers are a simple, low-cost and effective alternative for harnessing this broadly existing mechanical energy source, Wang says.

The UW-Madison team’s advance is the latest in a green energy research field called “roadside energy harvesting” that could, in some settings, rival solar power — and it doesn’t depend on fair weather. Researchers like Wang who study roadside energy harvesting methods see the ground as holding great renewable energy potential well beyond its limited fossil fuel reserves.

“Roadside energy harvesting requires thinking about the places where there is abundant energy we could be harvesting,” Wang says. “We’ve been working a lot on harvesting energy from human activities. One way is to build something to put on people, and another way is to build something that has constant access to people. The ground is the most-used place.”

Heavy traffic floors in hallways and places like stadiums and malls that incorporate the technology could produce significant amounts of energy, Wang says. Each functional portion inside such flooring has two differently charged materials — including the cellulose nanofibers, and would be a millimeter or less thick. The floor could include several layers of the functional unit for higher energy output.

“So once we put these two materials together, electrons move from one to another based on their different electron affinity,” Wang says.

The electron transfer creates a charge imbalance that naturally wants to right itself but as the electrons return, they pass through an external circuit. The energy that process creates is the end result of TENGs.

Wang says the TENG technology could be easily incorporated into all kinds of flooring once it’s ready for the market. Wang is now optimizing the technology, and he hopes to build an educational prototype in a high-profile spot on the UW-Madison campus where he can demonstrate the concept. He already knows it would be cheap and durable.

“Our initial test in our lab shows that it works for millions of cycles without any problem,” Wang says. “We haven’t converted those numbers into year of life for a floor yet, but I think with appropriate design it can definitely outlast the floor itself.”

The Wisconsin Alumni Research Foundation holds the patent to the technology. Other authors on the paper include Zhiyong Cai of the Forest Products Laboratory and UW-Madison graduate students Alberto Hernandez and Yanhao Yu. The Forest Products Laboratory and National Science Foundation provided funding for the research.

—Will Cushman