Forest Products Laboratory’s (FPL) researcher James Wacker with collaborators from the Department of Civil Environmental Engineering, South Dakota State University are working on a new approach to inspecting bridges that will allow inspections to one day be more cost-efficient, easier to conduct, more accessible, and safer for motorists and inspectors alike. The journal article, “New Bridge Inspection Approach with Joint UAV and DIC System,” was published in Structures Congress 2020.
Our nation’s bridges have been under an every-two-year mandated inspection for nearly 50 years. The current method of inspecting bridges is accomplished largely by visual assessment often using costly snooper trucks. Wacker describes this approach as “a passive approach that has provided subjective and unreliable data.”