Repaving a parking lot isn’t generally something we’d get too excited about here at the Forest Products Laboratory (FPL). That is, unless the project incorporates wood, in which case, we’re totally stoked.

Test site for cellulose nanomaterial-enhanced concrete in Greenville, S.C. Photo credit: Michael Goergen

And that’s exactly what happened in Greenville, South Carolina, at the headquarters for the U.S. Endowment for Forestry and Communities (Endowment). A parking lot there has become the largest test site in the world for cellulose nanomaterial (CN)-enhanced concrete, which FPL researchers and partners at the Endowment, Oregon State University, and Purdue University have found to have improved properties over traditional concrete.