Almost Famous FPL Research Heads to Hollywood

FPL research led to the creation of Hollywood’s first 100 percent sustainable studio set.

FPL research led to the creation of Hollywood’s first 100 percent sustainable studio set.

Hollywood’s first 100 percent sustainable studio set was created for 20th Century Fox’s  comedy series “Raising Hope” thanks to the efforts of the Forest Products Laboratory and NOBLE Environmental Technologies (NET).

The set was created using ECOR, a strong, light-weight bio-based panel.

The set was created using ECOR, a strong, light-weight bio-based panel.

Much of the set was created using ECOR®, a strong, light-weight bio-based panel that was developed through the collaborative efforts of FPL and NET. The project is also featured on the USDA Blog.

A recent San Diego KUSI-TV morning show segment also featured ECOR® technology. Bob Noble, founder of NET, talks about how his company partnered with USDA to develop a valuable, sustainable product that promotes job growth in the San Diego area.

Bob Noble, founder of NET.