Bilek, E.M. (Ted); Skog, Kenneth E.; Fried, Jeremy; Christensen, Glenn. 2005.
Fuel to burn: Economics of converting forest thinnings to energy using BioMax in Southern Oregon. Gen. Tech. Rep. FPL-GTR-157. Madison, WI: U.S. Department of Agriculture, Forest Service, Forest Products Laboratory. 27 p.